Stainless steel is categorized into different grades depending upon the elements added to it and the properties inherited by it. Stainless Steel 347 Sheet is one such sheet that has inherited certain properties of stainless steel. Stainless Steel 347 Plate offer resistance to heat and corrosion. ASTM A240 Type 347 are non-magnetic in nature and have high strength.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 347 sheet in China. If you're going to wholesale high quality stainless steel 347 sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Stainless steel is categorized into different grades depending upon the elements added to it and the properties inherited by it. Stainless Steel 347 Sheet is one such sheet that has inherited certain properties of stainless steel. Stainless Steel 347 Plate offer resistance to heat and corrosion. ASTM A240 Type 347 are non-magnetic in nature and have high strength.

4 223

These ASTM A240 Grade 347 have a stable design and superior construction. 347 Stainless Steel Plate produced by us are accurate in dimension and have a precise design. 347 Stainless Steel Sheet also offers good resistance in strong oxidizing conditions. 

 

Grade C (Carbon) Ni (Nickel) Si (Silicon) N (Nitrogen) S (Sulfur) Mn (Manganese) P (Phosphorus) Cr (Chromium) Mo (Molybdenum)
SS 347 (Min) - 9.00 - - - - - 17.0 2.00
SS 347 (Max) 0.08 13.00 1.00 - 0.030 2.00 0.045 20.0 3.00

Even after exposure to a temperature that is prone to carbide precipitation 347 2b, Stainless Steel Sheet offers resistance to intergranular corrosion. SS 347 Plate also displays creep resistance at 1500 degrees C. A240 GR 347 Rolling Plate display excellent toughness at low temperature. SA240 347 Clad Plate cannot be hardened by heat treatment and require cold working for hardening.

4 360

AISI 347 EN 1.4961 Rolling Sheet is used in chemical processing, food processing, waste heat recovery recuperation, and so on. ASTM A240 347 Perforated Platecan be used in nitric solution, organic acids in moderate temperature, and phosphoric acid in low temperature. 

 

347 Stainless Steel Coil can also be used in chloride or fluoride-free caustic solutions. Conventional methods of welding are used in fabricating 347 Stainless Steel Strip. Work hardening of ASTM A240 Type 347 Shim Stock is not recommended below 1700 degrees F. the material used in 347 2b Stainless Steel Flat Sheet needs to be annealed after working.

 

This helps the A240 Tp347 Slit Coil in reattaining the maximum resistance to corrosion. The alloy used in UNS S34709 Plate manufacturing is said to be ductile and easy to form. 347 Stainless Steel Polished Plate may not be treated with heat post welding. Our team of experts has been keeping in mind all these characteristics of A240 Tp 347 Hot rolled Plate while recommending them to our customers.