Alloy 316/316L Stainless Steel Sheet
video

Alloy 316/316L Stainless Steel Sheet

Alloy 316/316L (UNS S31600/S31603) is a chromium-nickelmolybdenum austenitic stainless steel developed to provide improved corrosion resistance to Alloy 304/304L in moderately corrosive environments. It is often utilized in process streams containing chlorides or halides. The addition of molybdenum improves general corrosion and chloride pitting resistance. It also provides higher creep, stress-to-rupture and tensile strength at elevated temperatures.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 316/316l stainless steel sheet in China. If you're going to wholesale high quality alloy 316/316l stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 316/316L (UNS S31600/S31603) is a chromium-nickelmolybdenum austenitic stainless steel developed to provide improved corrosion resistance to Alloy 304/304L in moderately corrosive environments. It is often utilized in process streams containing chlorides or halides. The addition of molybdenum improves general corrosion and chloride pitting resistance. It also provides higher creep, stress-to-rupture and tensile strength at elevated temperatures.

 

It is common practice for 316L to be dual certified as 316 and 316L. The low carbon chemistry of 316L combined with an addition of nitrogen enables 316L to meet the mechanical properties of 316.

4 237

Property 316 Stainless Steel Sheet 316L Stainless Steel Sheet
Density 8.0 g/cm³ 8.0 g/cm³
Melting Range 2500 – 2550°F (1371 – 1399°C) 2500 – 2550°F (1371 – 1399°C)
Tensile Strength 75 ksi (515 MPa) 70 ksi (485 MPa)
Yield Strength 30 ksi (205 MPa) 25 ksi (170 MPa)
Elongation 40% 40%
Corrosion Resistance Excellent in a wide range of environments Excellent, particularly resistant to intergranular corrosion
Applications Marine, chemical processing, medical devices Chemical process equipment, storage tanks, marine applications

Alloy 316/316L resists atmospheric corrosion, as well as, moderately oxidizing and reducing environments. It also resists corrosion in polluted marine atmospheres. The alloy has excellent resistance to intergranular corrosion in the as-welded condition. Alloy 316/316L has excellent strength and toughness at cryogenic temperatures.

 

Alloy 316/316L is non-magnetic in the annealed condition, but can become slightly magnetic as a result of cold working or welding. It can be easily welded and processed by standard shop fabrication practices.

Hot Tags: alloy 316/316l stainless steel sheet, China alloy 316/316l stainless steel sheet suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate, 400 2 4360 Alloy Pipe, SS409 Stainless Steel Welded Pipe