Stainless 321 Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless 321 steel plate in China. If you're going to wholesale high quality stainless 321 steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Introduction to 321 Stainless Steel Plate:
321 stainless steel is a versatile austenitic stainless steel alloy known for its excellent corrosion resistance, high strength, and heat resistance. It contains titanium, which stabilizes the alloy against chromium carbide precipitation resulting from welding or high-temperature exposure. 321 stainless steel plate finds widespread applications across industries where corrosion resistance and heat resistance are essential.

Key Features:
Corrosion Resistance: 321 stainless steel plate offers exceptional resistance to corrosion in a wide range of environments, including aqueous solutions of organic and inorganic acids. Its corrosion resistance is further enhanced by the addition of titanium, which stabilizes the alloy against chromium carbide precipitation.
High Temperature Resistance: One of the key features of 321 stainless steel is its high temperature resistance. It maintains good mechanical properties at elevated temperatures, making it suitable for applications involving exposure to high temperatures, such as exhaust systems, jet engine parts, and heat exchangers.

Applications:
Chemical Processing: In chemical processing industries, 321 stainless steel is utilized in reactors, vessels, and piping systems handling corrosive chemicals. Its corrosion resistance and heat resistance make it ideal for applications where exposure to corrosive environments and high temperatures is inevitable.
Automotive: 321 stainless steel plate is used in automotive exhaust systems, where its high temperature resistance and corrosion resistance are crucial for durability and performance. It is also employed in other automotive components requiring resistance to corrosive environments.
Specifications:
| Specification | Description |
|---|---|
| Thickness | 0.1 mm - 10 mm |
| Width | 100 mm - 2000 mm |
| Length | Customized |
| Surface Finish | Cold Rolled, Hot Rolled, Annealed, Pickled, Bright Annealed |
| Material | 321 Stainless Steel Alloy |
| Strength | ≥ 515 MPa |
| Tensile Strength | ≥ 740 MPa |
| Yield Strength | ≥ 205 MPa |
| Density | 7.93 g/cm³ |
| Melting Point | 1398-1446°C |
| Corrosion Resistance | Excellent resistance to organic and inorganic acids, high temperature oxidation |
| Typical Applications | Aerospace, Chemical Processing, Automotive |
| Manufacturing Standards | ASTM A240, ASME SA240 |
In summary, 321 stainless steel plate offers exceptional corrosion resistance, high temperature resistance, and weldability, making it a preferred choice for critical applications across aerospace, chemical processing, and automotive industries.
Hot Tags: stainless 321 steel plate, China stainless 321 steel plate suppliers, SS431 Stainless Steel Plate, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, 1 4510 Stainless Steel Patterned Plate, Corrugated SS Roof Sheet