316/316L Stainless Alloy Plate
video

316/316L Stainless Alloy Plate

Alloys 316 (UNS S31600) and 316L (UNS S31603) are molybdenum-bearing austenitic stainless steels, which are more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels such as Alloy 304. These alloys also offer higher creep, stress-to-rupture, and tensile strength at elevated temperatures. In addition to excellent corrosion resistance and strength properties, the Alloys 316 and 316L Cr-Ni-Mo alloys also provide excellent fabricability and formability which are typical of the austenitic stainless steels.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316/316l stainless alloy plate in China. If you're going to wholesale high quality 316/316l stainless alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloys 316 (UNS S31600) and 316L (UNS S31603) are molybdenum-bearing austenitic stainless steels, which are more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels such as Alloy 304. These alloys also offer higher creep, stress-to-rupture, and tensile strength at elevated temperatures. In addition to excellent corrosion resistance and strength properties, the Alloys 316 and 316L Cr-Ni-Mo alloys also provide excellent fabricability and formability which are typical of the austenitic stainless steels.

4 231

  Composition (Weight Percent)   CCT2 CPT3
ALLOY Cr Mo N PREN1 °F (°C) °F (°C)
Type 304 18.0 - 0.06 19.0 <27.5
(<-2.5)
-
-
Type 316 16.5 2.1 0.05 24.2 27.5
(-2.5)
59
(15.0)
Type 317 18.5 3.1 0.06 29.7 35.0
(1.7)
66
(18.9)
SSC-6MO 20.5 6.2 0.22 44.5 110
(43.0)
149
(65)

Hot Tags: 316/316l stainless alloy plate, China 316/316l stainless alloy plate suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS431 Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate