SS 302 Stainless Steel
video

SS 302 Stainless Steel

Type 302 Stainless Steel is an austenitic chromium-nickel stainless steel, non-hardenable by thermal treatments. It may be cold worked to high tensile strengths with slightly lower ductility than Type 301. Its corrosion resistance is superior to that of Type 301. Type 302 is essentially nonmagnetic in the annealed condition and becomes slightly magnetic when cold worked.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 302 stainless steel in China. If you're going to wholesale high quality ss 302 stainless steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Type 302 Stainless Steel is an austenitic chromium-nickel stainless steel, non-hardenable by thermal treatments. It may be cold worked to high tensile strengths with slightly lower ductility than Type 301. Its corrosion resistance is superior to that of Type 301. Type 302 is essentially nonmagnetic in the annealed condition and becomes slightly magnetic when cold worked.

4 307

Feature Description
Grade SS302
Standard ASTM A240 / ASME SA240
Thickness 0.3 mm to 150 mm
Width 1000 mm, 1219 mm, 1500 mm, 2000 mm, 2500 mm, 3000 mm, Custom sizes available
Length 2000 mm, 2440 mm, 3000 mm, 6000 mm, Custom sizes available
Element Type
Carbon 0.15 max.
Manganese 2.00 max.
Sulfur 0.030 max.
Phosphorus 0.045 max.
Silicon 0.75 max.
Chromium 17.00 -19.00
Nickel 8.00 – 10.00
Nitrogen 0.10 max.

 

Hot Tags: ss 302 stainless steel, China ss 302 stainless steel suppliers, SS409 Stainless Steel Welded Pipe, SS410 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet, Stainless Steel 316 316L 316Ti Sheets And Plates