904L Stainless Steel Plate&Sheet
video

904L Stainless Steel Plate&Sheet

904L was originally developed to withstand environments containing dilute sulfuric acid, and is one of the few stainless steels that, at temperatures up to 95°F (35°C), provides full resistance in such environments within the entire concentration range of 0 to 100%. 904L also offers good resistance to a number of other inorganic acids, such as phosphoric acid and most organic acids. However, acids and acid solutions containing halide ions can be very aggressive, and the corrosion resistance of 317L, 317LMN and 904L may be insufficient.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 904l stainless steel plate&sheet in China. If you're going to wholesale high quality 904l stainless steel plate&sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

The high content of alloying elements in 904L gives the alloy exceptionally good resistance to uniform corrosion.

 

Alloy 904L is a high-alloy austenitic stainless steel known for its exceptional corrosion resistance in aggressive environments. This material is particularly effective against sulfuric acid and chloride attack, making it suitable for use in harsh conditions where other stainless steels may fail. Alloy 904L combines molybdenum and copper, enhancing its ability to resist pitting and crevice corrosion.

4 226

Specification Details
Standard ASTM B625, ASME SB625, EN 10088-2, DIN 1.4539
Grade 904L (UNS N08904)
Thickness 0.1mm - 100mm
Width 1000mm - 2000mm
Length 2000mm - 6000mm
Surface Finish No.1, 2B, No.4, HL, BA, Mirror
Edge Finish Mill Edge, Slit Edge
Heat Treatment Solution Annealed

Fractional distillation of tall oil often needs better material than 316L or even the more frequently used 317LMN. In these hot concentrated caustic solutions, the corrosion resistance is mainly determined by the nickel content of the material. With a nickel content of 25%, 904L has proven to be a good alternative to most conventional stainless steels.

 

Conventional stainless steels such as 304L and 316L are susceptible to chloride stress corrosion cracking (SSC) under certain conditions. Resistance to SSC increases with the increased content of nickel and molybdenum. Therefore, the higher performance austenitic stainless steels such as 904L have very good resistance to SSC. The table in the upper right corner shows resistance to SSC in a chloride solution under evaporative conditions. High performance austenitic steels and duplex stainless steels clearly outperform 316L.

Hot Tags: 904l stainless steel plate&sheet, China 904l stainless steel plate&sheet suppliers, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet, 400 2 4360 Alloy Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates