904L Stainless Steel Medium Thick Plate
video

904L Stainless Steel Medium Thick Plate

Alloy 904L (UNS N08904) is a super austenitic stainless steel that is designed for moderate to high corrosion resistance in a wide range of process environments. The combination of high chromium and nickel content, coupled with additions of molybdenum and copper, assure good to excellent corrosion resistance.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 904l stainless steel medium thick plate in China. If you're going to wholesale high quality 904l stainless steel medium thick plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 904L (UNS N08904) is a superaustenitic stainless steel that is designed for moderate to high corrosion resistance in a wide range of process environments. The combination of high chromium and nickel content, coupled with additions of molybdenum and copper, assure good to excellent corrosion resistance.

With its highly alloyed chemistry - 25% nickel and 4.5% molybdenum, 904L provides good chloride stress corrosion cracking resistance, pitting and general corrosion resistance superior to 316L and 317L molybdenum enhanced stainless steels.

Alloy 904L was originally developed to withstand environments containing dilute sulfuric acid. It also offers good resistance to other inorganic acids such as hot phosphoric acid as well as most organic acids.

Alloy 904L is easily welded and processed by standard shop fabrication practices.

product-750-750product-750-750product-750-750product-750-750

 

The high content of alloying elements in 904L gives the alloy exceptionally good resistance to uniform corrosion.

904L was originally developed to withstand environments containing dilute sulfuric acid, and is one of the few stainless steels that, at temperatures up to 95°F (35°C), provides full resistance in such environments within the entire concentration range of 0 to 100%. 904L also offers good resistance to a number of other inorganic acids, such as phosphoric acid and most organic acids. However, acids and acid solutions containing halide ions can be very aggressive, and the corrosion resistance of 317L, 317LMN and 904L may be insufficient.

Fractional distillation of tall oil often needs better material than 316L or even the more frequently used 317LMN. In these hot concentrated caustic solutions, the corrosion resistance is mainly determined by the nickel content of the material. With a nickel content of 25%, 904L has proven to be a good alternative to most conventional stainless steels.

Conventional stainless steels such as 304L and 316L are susceptible to chloride stress corrosion cracking (SSC) under certain conditions. Resistance to SSC increases with the increased content of nickel and molybdenum. Therefore, the higher performance austenitic stainless steels such as 904L have very good resistance to SSC. The table in the upper right corner shows resistance to SSC in a chloride solution under evaporative conditions. High performance austenitic steels and duplex stainless steels clearly outperform 316L.

Mechanical Properties

Typical Values at 68°F (20°C) (minimum values, unless specified)

Yield Strength
0.2% Offset
Ultimate Tensile
Strength
Elongation
in 2 in.
Hardness
psi (min.) (MPa) psi (min.) (MPa) % (min.) (max.)
31,000 220 71,000 490 36 70-90 Rockwell B

 

Chemical Analysis

Weight % (all values are maximum unless a range is otherwise indicated)

       
Nickel 23.0 min.-28.0 max. Silicon 1.00
Chromium 19.0 min.-23.0 max. Phosphorus 0.045
Molybdenum 4.0 min.-5.0 max. Sulfur 0.035
Copper 1.0-2.0 max. Iron Balance
Manganese 2.00  

 

 

FAQ

 

Q: Can I get your best price?

A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.

Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.
Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable

Hot Tags: 904l stainless steel medium thick plate, China 904l stainless steel medium thick plate suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, 400 2 4360 Alloy Pipe, SS409 Stainless Steel Welded Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet, 1 4510 Stainless Steel Patterned Plate