304/304L Stainless Steel Plate
video

304/304L Stainless Steel Plate

Alloy 304/304L has good resistance to atmospheric corrosion, foods and beverages and to many organic and inorganic chemicals in moderately oxidizing to moderately reducing environments. The high chromium content of the alloy provides resistance to oxidizing solutions such as nitric acid up to 55% weight and up to 176°F (80°C).
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 304/304l stainless steel plate in China. If you're going to wholesale high quality 304/304l stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 304/304L has good resistance to atmospheric corrosion, foods and beverages and to many organic and inorganic chemicals in moderately oxidizing to moderately reducing environments. The high chromium content of the alloy provides resistance to oxidizing solutions such as nitric acid up to 55% weight and up to 176°F (80°C).

4 176

Alloy 304/304L also resists moderately aggressive organic acids such as acetic. The nickel present in the alloy provides resistance to moderately reducing solutions such as pure phosphoric acid, whatever the concentration, in cold solutions and up to 10% diluted hot solutions. The alloy can also operate successfully in caustic solutions free of chlorides or Alloy 304/304L does not perform well in more highly reducing environments such as those containing chlorides and sulfuric acid.

Temperature Range  
°F °C in/in °F cm/cm °C
68-212 20-100 9.2 x 10-6 16.6 x 10-6
68-932 20-500 10.6 x 10-6 18.2 x 10-6
68-1600 20-870 11.0 x 10-6 19.8 x 10-6

304 Stainless Steel Plate: Known for its versatility and excellent corrosion resistance, making it ideal for a variety of applications including kitchen equipment and chemical containers.

 

304L Stainless Steel Plate: Similar to 304 but with a lower carbon content, which enhances its corrosion resistance after welding or stress relieving, making it suitable for chemical processing and other high-corrosion environments.

Hot Tags: 304/304l stainless steel plate, China 304/304l stainless steel plate suppliers, SS410 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet