0.5*1240x2440mm Stainless Steel Smooth Mirror Sheet Panel Ti-Gold Mirror Plate
video

0.5*1240x2440mm Stainless Steel Smooth Mirror Sheet Panel Ti-Gold Mirror Plate

Product Specifications 1)Thickness: 0.15 to 80mm 2)Width: 10-1525mm 3)Grade:201,301,304,304L,316,316L,410,430 4)Surface: NO. 1, 2B, BA, NO. 3, NO. 4, HL, NO. 8 and so on 5)Color :Champagne, rose gold, rose red, coffee gold, black gold, brown, black, red copper, antique copper, brass, titanium, grey, violet, bronze, sapphire, jade green, etc. 6)Pattern : Linen,cubes,diamond,panda,bamboo,water wave, etc. 7)Anti-fingerprint available. 8)PVC film details,Laser PVC, POLI-FILM , NOVANCEL, PVC thickness 70 -100 Micron Laser PVC, Single/Double 70 Micron Black&white PVC 9)Use:Decoration, Elevator, Electric Appliance, Door
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 0.5*1240x2440mm stainless steel smooth mirror sheet panel ti-gold mirror plate in China. If you're going to wholesale high quality 0.5*1240x2440mm stainless steel smooth mirror sheet panel ti-gold mirror plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

0.5*1240x2440mm Stainless Steel Smooth Mirror Sheet Panel Ti-Gold Mirror Plate

Description

Loading Port: Shanghai Length: 2000mm-6000mm
Oem/Odm: Acceptable Service: Cutting, Surface Treatment
Technique: Cold Rolled Tolerance: ±1%
Wdith: 10-2000mm Hardness: Hard
Price Term: L/C T/T (30% Deposit) Standard: ASME, ASTM, EN ,BS,GB,DIN, JIS Etc

0.5*1240x2440mm Stainless Steel Smooth Mirror Sheet Panel Ti-Gold Mirror Plate

 

Product Specifications
1)Thickness: 0.15 to 80mm
2)Width: 10-1525mm
3)Grade:201,301,304,304L,316,316L,410,430
4)Surface: NO. 1, 2B, BA, NO. 3, NO. 4, HL, NO. 8 and so on
5)Color :Champagne, rose gold, rose red, coffee gold, black gold, brown, black, red copper, antique copper, brass, titanium, grey, violet, bronze, sapphire, jade green, etc.
6)Pattern : Linen,cubes,diamond,panda,bamboo,water wave, etc.
7)Anti-fingerprint available.
8)PVC film details,Laser PVC, POLI-FILM , NOVANCEL, PVC thickness 70 -100 Micron Laser PVC, Single/Double 70 Micron Black&white PVC
9)Use:Decoration, Elevator, Electric Appliance, Door

After Service Concept
The first customers become lifelong customers.
If you want to purchase some products to test the market, we can lower the MOQ
Delivery: Normally 15-20 days
Productivity: 7000-8000 tons/month
Packing: Standard export sea-worthy packing in wooden pallet.
 

Chemical Composition

Grade STS304 STS 316 STS430 STS201
Elong(10%) Above 40 30MIN Above 22 50-60
Hardness ≤200HV ≤200HV Below 200 HRB100,HV 230
Cr(%) 18-20 16-18 16-18 16-18
Ni(%) 8-10 10-14 ≤0.60% 0.5-1.5
C(%) ≤0.08 ≤0.07 ≤0.12% ≤0.15

 

0.5*1240x2440mm  Stainless Steel Smooth Mirror Sheet Panel  Ti-Gold Mirror  Plate 0

QING SHAN is the more than 10 years professional manufactory, a large integrated Enterprise of stainless steel material's design,processing and marketing,various kinds of decorative stainless steel products such as Hairline/No.4,Super Mirror /etched/embossed /Color,etc.
================================================================================
Why do you choose us ?
· We have high reputation based on best quality products,To guarantee the quality of the products we can meet most of the standards all over the world such as ASTM standard.
· We can offer competitive price for your buiness,we are one of the biggest stainless steel sheets stock holder in Foshan
· Our after-sell service team will help you solving all the related problems ;
· Shortest and stable delivery time;
· We can provide stainless steel processing services.All of our products are produce by our professional workman and we have our high-work-effect foreign trade team, you can totally believe our service.
.Flexible payment options such us:TT/ LC, Western union ,MoneyGraim and Sale on credit for regular buyers.
==================================================================================
FAQ:
1.How does your company do regarding quality control?
All our final products before shipment are strongly required to adhere to ISO9001 quality management standard. While applying good quality control system, in China
2.What is the MOQ?
1-30pcs,base on different pattern.
3.What is the delivery ?
Normaly within 7-25 days, According to the sizes and Qty.
4.How many coutries you already exported ?
We haved exported to over 30 coutries, mainly in, Middle East, Asia, Europe
5.How can I get some samples?
Through the international express delivery,like UPS,DHL,TNT and so on.

 

Hot Tags: 0.5*1240x2440mm stainless steel smooth mirror sheet panel ti-gold mirror plate, China 0.5*1240x2440mm stainless steel smooth mirror sheet panel ti-gold mirror plate suppliers, Corrugated SS Roof Sheet, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry