The high nickel and chromium content of Alloys 800H and 800HT generally means they will have very similar aqueous corrosion resistance. The alloys have corrosion resistance that is comparable to 304 when used in nitric and organic acid service. The alloys should not be used in sulfuric acid service. They are subject to chromium carbide precipitation if in service for prolonged exposure in the 1000-1400°F (538-760°C) temperature range.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of heat resistant alloy 800 / 800h stainless steel plate thickness 0.6 - 20.0mm plate in China. If you're going to wholesale high quality heat resistant alloy 800 / 800h stainless steel plate thickness 0.6 - 20.0mm plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

eat Resistant Alloy 800 / 800H Stainless Steel Plate Thickness 0.6 - 20.0mm in Stock

 

Products 416 stainless steel sheet
Thickness 0.3 - 4.0mm
Width 1000mm 1219mm 1500mm or as request
Standard ASTM A240/240M-18
Brand TISCO BAOSTEEL POSCO
Service Cutting , bending , surface finishing
Other Grade 201 202 304 304L 304H 309S 310S 316L 316Ti 317L 321 347 410 420 430 431 444,2205 2507 904L 254SMO 253MA N08020 C276 625 600 800 825 monel 400 500.etc
Standard Size 1000*2000mm 1219*2438mm 1500*6000mm

 

Material Description of Alloy 800/800H

 

Alloys 800H (UNS N08810) and 800HT (UNS N08811) are dual-certifiable Nickel-Iron-Chromium materials that resist oxidation, carburization and other high temperature corrosion. The chemical composition of the two alloys are identical to Alloy 800 (UNS N08800), with the exception of the higher level of carbon present in both grades- (0.05–0.10%) in alloy 800H, and (0.06–0.10%) in alloy 800HT. Alloy 800HT also has an addition of up 1.0 % aluminum and titanium. In addition to the chemistry restrictions, both alloys receive a high temperature annealing treatment that produces an average grain size of ASTM 5 or coarser. The restricted chemical compositions, combined with the high temperature anneal, assure these materials have greater creep and rupture strength when compared to Alloy 800.

 

Alloy 800H has good creep-rupture properties at temperatures above 1100°F (600°C). It remains ductile during long term use at temperatures below 1290°F (700°C) due to a maximum titanium and aluminum content of 0.7%. Alloy 800 with a standard anneal is recommended for service below 1100°F (600°C). Alloy 800H resists reducing, oxidizing and nitriding atmospheres, as well as, atmospheres that alternate between reducing and oxidizing. The alloy remains stable in long term high temperature service.

 

Alloy 800HT has excellent creep strength at temperatures above 1290°F (700°C). If the application involves frequent temperature excursions under 1290°F (700°C) or parts of are permanently exposed to a temperature below 1290°F (700°C), Alloy 800H should be utilized. The high temperature resistance of Alloy 800HT is comparable to Alloy 800H. It also remains stable in long term high temperature service.

 

Chemical Analysis of Alloy 800 / 800H

 

Weight % (all values are maximum unless a range is otherwise indicated)

Element 800H 800HT
Nickel 30.0 min.-35.0 max. 30.0 min.-35.0 max.
Chromium 19.0 min.-23.0 max. 19.0 min.-23.0 max.
Iron 39.5 39.5
Carbon 0.05 min.-0.10 max. 0.06 min.-0.10 max.
Manganese 1.50 1.50
Phosphorus 0.045 0.045
Sulfur 0.015 0.015
Silicon 1.0 1.0
Aluminum 0.15 min.-0.60 max. 0.25 min.-0.60 max.
Titanium 0.15 min.-0.60 max. 0.25 min.-0.60 max.
Aluminum & Titanium 0.30 min.-1.20 max. 0.85 min.-1.20 max.

 

Corrosion Resistance of 800 / 800H Alloy

 

The high nickel and chromium content of Alloys 800H and 800HT generally means they will have very similar aqueous corrosion resistance. The alloys have corrosion resistance that is comparable to 304 when used in nitric and organic acid service. The alloys should not be used in sulfuric acid service. They are subject to chromium carbide precipitation if in service for prolonged exposure in the 1000-1400°F (538-760°C) temperature range.

Since Alloys 800H and 800HT were developed primarily for hightemperature strength, corrosive environments to which these grades are exposed normally involve high temperature reactions such as oxidation and carburization.

 

Application of 800/800H alloy

Chemical and Petrochemical Processing-process equipment for the production of ethylene, ethylene dichloride, acetic anhydride, ketene, nitric acid and oxy-alcohol

Petroleum Refining-steam/hydrocarbon reformers and hydrodealkylation units

Power Generation-steam super-heaters and high temperature heat exchangers in gas-cooled nuclear reactors, heat exchangers and piping systems in coal-fired power plants

Thermal Processing Fixtures-radiant tubes, muffles, retorts and fixtures for heat-treating furnaces

Heat Resistant Alloy 800 / 800H Stainless Steel Plate Thickness 0.6 - 20.0mm plate 4

Hot Tags: heat resistant alloy 800 / 800h stainless steel plate thickness 0.6 - 20.0mm plate, China heat resistant alloy 800 / 800h stainless steel plate thickness 0.6 - 20.0mm plate suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 400 2 4360 Alloy Pipe, 1 4510 Stainless Steel Patterned Plate, SS431 Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry