SS 310H Stainless Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 310h stainless steel plate in China. If you're going to wholesale high quality ss 310h stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SS 310H Sheets usually manufactured with superior grade material. The variations have different dimensions and tolerances for flatness, shapes, efficiency, and other properties. All of these features including mechanical and thermal characteristics of SS 310 material are retained by our products following the standard formats.

SS 310 is proposed for high temperature with austenitic structure. These steel grade are chromium enhanced nickel-carbon composition to obtain better corrosion resistance. Carbon content defines SS 310 modification in SS 310S with decreasing value and SS 310H with increasing value.
| Specification | Description |
|---|---|
| Standard | ASTM A240 / ASME SA240 |
| Dimension Standard | MSRR, AMS, BS, JIS, AISI, ASTM, GB, DIN, EN, etc |
| Thickness (SS 310S) | 0.3 mm to 120 mm |
| Width (SS 310H) | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
| Length (SS 310) | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc |
| Finish | 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc. |
| Hardness (SS 310S) | Half Hard, Soft, Hard, Quarter Hard, Spring Hard |
| Profiling | Plasma Plate Cutting, Laser Plate Cutting, Oxy-propane Flame Cutting |
SS 310S plate is preferred in sulphides and also reduces carburizing at higher temperatures due to low carbon. SS 310H plates are boosted to higher strength and toughness. Plates are manufactured in various forms and thicknesses to gain required hardness. SS 310 plates are frequently used in high stress conditions with improved tensile strength.

Our SS 310H Sheets gives special protection from the full scope of corrosion media, such as particle stress cracking and appropriate for the high temperature. Our SS 310 Sheets offer protection from oxidation, and sheets, plates can be used at cryogenic temperatures.
SS 310S Sheets and Plates are open in both reliable and welded structures in different sizes. Our high-grade Sheets and Plates has bewildering durability at high temperatures. So these are the unique reasons we have huge demands in industries, and it helps us to manufacture the more attractive products.
Hot Tags: ss 310h stainless steel plate, China ss 310h stainless steel plate suppliers, SS431 Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates