ASTM AISI Alloy Steel Plate 4140 JIS SCM440 DIN 42CrMo4 DIN 1.7225 4' X 8' X 50 Mm
video

ASTM AISI Alloy Steel Plate 4140 JIS SCM440 DIN 42CrMo4 DIN 1.7225 4' X 8' X 50 Mm

All common arc welding processes, such as (SAW, SMAW, FCAW, GMAW, GTAW) can be used to weld 4140 alloy steel, but in order to prevent cracking, it must be preheated to 170-350 °C (350-650 °F) before welding, preheating interpass temperature depends on the section thickness of the steel.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm aisi alloy steel plate 4140 jis scm440 din 42crmo4 din 1.7225 4' x 8' x 50 mm in China. If you're going to wholesale high quality astm aisi alloy steel plate 4140 jis scm440 din 42crmo4 din 1.7225 4' x 8' x 50 mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM AISI Alloy Steel Plate 4140 JIS SCM440 DIN 42CrMo4 DIN 1.7225 4' X 8' X 50 Mm

Description

Technique: Hot Rolled Standard: ASTM,AISI,JIS,DIN
Length: 1000-12000mm Type: Steel Plate
Width: 2000-2300mm,1000mm-2000mm Special Use: Alloy Structual Steel
Grade: Alloy Steel Plate 4140 Thickness: 1.2mm-400mm
Surface: Black Material: Alloy Structual Steel
Price Term: CIF,FOB,CFR
High Light:

ASTM AISI Alloy Steel Plate

,

DIN 1.7225 Alloy Steel Plate

,

4140 Alloy Plate

ASTM AISI 4140 JIS SCM440 DIN 42CrMo4 DIN1.7225 Alloy Steel Plate Size 4' x 8' x 50 mm

SAE AISI 4140 Alloy Steel

SAE 4140 (AISI 4140 steel) is a Cr-Mo series (Chrome molybdenum series) low alloy steel, the material has high strength and hardenability, good toughness, small deformation during quenching, high creep strength and long-lasting strength at high temperature.

4140 Steel Uses

AISI SAE 4140 alloy steel can be made into round steel bar, flat & square steel bar, steel plate, steel tube, and has many uses in the aerospace, oil and gas and automotive industries, typical uses are thin-walled pressure vessels, forged gears and shafts (Motor shafts, pump shafts, hydraulic shafts, etc.), spindles (lathe spindles, milling spindles, etc.), collars, clamps, high strength bolts, valve bonnet, screws, nuts, worms, collets, torsion bars and various carburized parts.

Datasheet & Specification

Below are 4140 alloy steel datasheets including chemical composition, properties and equivalent chart, etc.

AISI SAE 4140 Chemical Composition

The table below lists AISI 4140 chemical composition.

  AISI SAE 4140 Chemical Composition (%)
Steel (UNS) C Si Mn P (≤) S (≤) Cr Mo Ni
4140 (G41400) 0.38-0.43 0.15-0.35 0.75-1.00 0.035 0.040 0.80-1.10 0.15-0.25 –

AISI 4140 Steel Mechanical Properties

Material 4140 mechanical properties are given in the table below.

Steel Tensile strength, Mpa (ksi) Yield strength, Mpa (ksi) Elongation in 50 mm (2 in), % Reduction in area, % Hardness (HB) Sample diameter Conditions
AISI 4140 1020 (148) 655 (95) 17.7 46.8 302 25.4mm (1 in.) Normalized at 870 °C (1600 °F)
655 (95) 414 (60) 25.7 56.9 197 Annealed at 815 °C (1500 °F)
1075 (156) 986 (143) 15.5 56.9 311 Water quenched from 845 °C (1550 °F) and tempered at 540 °C (1000 °F)

SAE 4140 Physical Properties

Notes: 10-6/K = 10-6.K-1 = (µm/m)/°C

Material 4140 coefficients of linear thermal expansion
Temperature, °C (°F) Value (10-6/K) Treatment or condition
20-100 (68-212) 12.2 Oil hardened, tempered
20-200 (68-392) 12.6
20-400 (68-752) 13.6
20-600 (68-1112) 14.5
4140 thermal conductivity
Value (W/m·K) Temperature, °C (°F) Treatment or condition
42.7 100 (212) Hardened &
tempered
42.3 200 (392)
37.7 400 (752)
33.1 600 (1112)
AISI / SAE 4140 Specific Heat
Value (J/Kg·K) Temperature, °C (°F) Treatment or condition
473 20-200 (68-392) Hardened &
tempered
519 20-400 (68-752)
561 20-600 (68-1112)
Mateiral 4140 Electrical Resistivity
Value (μΩ· m) Temperature, °C (°F) Treatment or condition
0.22 20 (68) Hardened &
tempered
0.26 100 (212)
0.33 200 (392)
0.48 400 (752)
0.65 600 (1112)

Material 4140 Steel Heat Treatment

The following table shows AISI 4140 steel heat treatment, Rockwell hardness.

Material 4140 Heat Treat Temperature, °C (°F) 4140 steel hardness Cooling/Agent
Normalizing 870 (1600) 302 HB Air
Annealing 790-845 (1455-1555) 197 HB Furnace cooling
Quenching 830-845 (1525-1555)   Oil
Tempering (2 hour) 205 (400) 58 HRC Oil hardening
260 (500) 54 HRC
315 (600) 50 HRC
370 (700) 47 HRC
425 (800) 45 HRC
480 (900) 40 HRC
540 (1000) 35 HRC
595 (1100) 33 HRC
650 (1200) 28 HRC

Normalizing

4140 alloy steel is typically normalized at 870 °C (1600°F), and should be cooled at a specified temperature in still air.

Spheroidizing Annealing

For spheroidizing annealing of 4140 alloy steel, it needs heat treated to 749 °C (1380 °F), followed by slowly cooling to 666 °C (1230 °F) at a rate of 6 °C (10 °F)/hour, or rapid cooling to 675 °C (1250 °F) for isothermal annealing.

Full Annealing

Heat treatment to 845 °C (1555 °F), slow cooling from 755 °C (1390 °F) at a rate of 14 °C (25 °F)/hour to 665 °C (1230 °F), or rapid cooling to 675 °C (1250 °F) for 5 hours isothermal annealing.

Tempering

Tempering temperature of 4140 alloy steel can be from 204-649 °C (400-1200°F) after normalizing and oil quenching, and the corresponding Rockwell hardness can be obtained.

Forging

Material 4140 forging temperature is about 1232 °C (2250 °F).

Welding of 4140 Steel

All common arc welding processes, such as (SAW, SMAW, FCAW, GMAW, GTAW) can be used to weld 4140 alloy steel, but in order to prevent cracking, it must be preheated to 170-350 °C (350-650 °F) before welding, preheating interpass temperature depends on the section thickness of the steel.

Equivalent Material

AISI 4140 equivalent material is listed in the table below.

AISI 4140 Equivalent Material
USA European Union China Japan ISO
Standard Grade (UNS) Standard Grade (Steel Number) Standard Grade Standard Grade Standard Grade
AISI SAE;
ASTM A29/A29M
4140 (G41400) EN 10083-3 42CrMo4 (1.7225) GB/T 3077 42CrMo JISG 4105 SCM440  

 

ASTM AISI Alloy Steel Plate 4140 JIS SCM440  DIN 42CrMo4 DIN 1.7225 4' X 8' X 50 Mm 0ASTM AISI Alloy Steel Plate 4140 JIS SCM440  DIN 42CrMo4 DIN 1.7225 4' X 8' X 50 Mm 1ASTM AISI Alloy Steel Plate 4140 JIS SCM440  DIN 42CrMo4 DIN 1.7225 4' X 8' X 50 Mm 2

Hot Tags: astm aisi alloy steel plate 4140 jis scm440 din 42crmo4 din 1.7225 4' x 8' x 50 mm, China astm aisi alloy steel plate 4140 jis scm440 din 42crmo4 din 1.7225 4' x 8' x 50 mm suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry