Cold Drawn ASTM A312 TP316L Stainless Steel Seamless Tube SS 316L Inox Tube
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of cold drawn astm a312 tp316l stainless steel seamless tube ss 316l inox tube in China. If you're going to wholesale high quality cold drawn astm a312 tp316l stainless steel seamless tube ss 316l inox tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Cold Drawn ASTM A312 TP316L Stainless Steel Seamless Tube SS 316L Inox Tube
Description
| Application: | Construction,Decoration,Industry,Chemical | Standard: | DIN,ASTM |
|---|---|---|---|
| Steel Grade: | 304 304L 316 316L 310S 321 | Type: | Seamless |
| Welding Line Type: | Seamless | Thickness: | 1-95mm |
| Length: | 3000mm~6000mm | Shape: | Round.square.Rectangle |
| Outer Diameter: | 6-762mm | ||
| High Light: |
TP316L Stainless Steel Seamless Tube,ASTM A312 Stainless Seamless Tube,1.5MM Stainless Steel Seamless Tube |
||
Product Description
Standard: ASTM A249, ASTM A268, ASTM A269, ASTM A312, etc.
Material: 316, 316L.
Item: Polished Bright Surface 316 316L welded stainless steel pipe for exhaust
Specification:
Outer diameter: 1.0-1220mm (1/8"-48")
Wall thickness: 0.1-150mm (SCH 5S- XXS)
Length: 3m, 5.8m, 6m, 11.8m, or as request.
Surface: Pickled, annealed, polished, bright, sand blast, hair line, etc.
What is 316?
Grade 316 is the standard molybdenum-bearing grade, second in importance to 304 amongst the austenitic stainless steels.
The molybdenum gives 316 better overall corrosion resistant properties than Grade 304, particularly higher resistance to pitting and crevice corrosion in chloride environments.
Grade 316L, the low carbon version of 316 and is immune from sensitisation (grain boundary carbide precipitation).
316/316L Chemical Composition
| Material | C | Si | Mn | P | S | Ni | Cr | Mo | N |
| 316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 10.0~14.0 | 16.0~18.0 | 2.00~3.00 | - |
| 316L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 10.0~14.0 | 16.0~18.0 | 2.00~3.00 | ≤0.10 |
316/316L Mechanical Properties
| Material |
Yield Strength N/mm2 |
Tensile Strength N/mm2 |
Elongation (%) |
| 316 | ≥205 | ≥515 | ≥35 |
| 316L | ≥170 | ≥485 | ≥35 |
Grade Specification Comparison
| Grade | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | Name | ||||
| 316L | S31603 | 316S11 | - | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
316/316L Stainless steel Applications
Typical applications include:
· Food preparation equipment particularly in chloride environments.
· Laboratory benches & equipment.
· Coastal architectural panelling, railings & trim.
· Boat fittings.
· Chemical containers, including for transport.
· Heat Exchangers.
· Woven or welded screens for mining, quarrying & water filtration.
· Threaded fasteners.
· Springs.
Production Process of stainless steel welded pipes

Products' Photos


Hot Tags: cold drawn astm a312 tp316l stainless steel seamless tube ss 316l inox tube, China cold drawn astm a312 tp316l stainless steel seamless tube ss 316l inox tube suppliers, Inconel 625 Alloy Steel Plate, Stainless Steel High Pressure Pipe, SS410 Stainless Steel Pipe, 410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, 1 4509 1 4510 Pipes And Tubes
You Might Also Like
Send Inquiry