Stainless Steel 904L Seamless Heat Exchanger Tubes
video

Stainless Steel 904L Seamless Heat Exchanger Tubes

SS 904L Heat Exchanger Tubes is utilized in many industrial applications. These heat exchanger/condensers are 904L grades stainless steel alloy product that includes a high amount of nickel and molybdenum content. Furthermore, it includes low carbon content and copper that ensures to improve...
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 904l seamless heat exchanger tubes in China. If you're going to wholesale high quality stainless steel 904l seamless heat exchanger tubes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS 904L Heat Exchanger Tubes is utilized in many industrial applications. These heat exchanger/condensers are 904L grades stainless steel alloy product that includes a high amount of nickel and molybdenum content. Furthermore, it includes low carbon content and copper that ensures to improve resistance to strong reducing acids. These are basically non-magnetic and exhibits superior formability and durability. The heat exchanger/ condensor possess superior sturdiness and toughness in hostile environments. The stainless steel alloy offers superior resistance to crevice and stress corrosion cracking.

 

Stainless Steel 904L Heat Exchanger Tubes Specification

Range : 10 mm OD to 50.8 mm OD

Outer Diameter : 6.00 mm to 101.60 mm

Wall Thickness : 0.70 mm to 8.00 mm

Length : up to 20 m (65.62 ft) Length & Customed Required Length

Specifications : ASTM A 213, A 268, A 269, A 789, Equivalent to ASME, EN, JIS Etc.

 

Standards for 904L Seamless Heat Exchanger Tubes

Material No. EN Designation UNS AISI/SAE
1.4539 X1NiCrMoCu25-20-5 N08904 904L

 

Mechanical Properties 20℃ Of 904L Seamless Tubes For Heat Exchanger Tubes

0.2% Yield Strength Rp≥N/mm2 Tensile Strength Rm N/mm2 Elongation A5
≥%
Modulus of Elasticity
kN/ mm2
230 530-730 35/30 195

 

Physical Properties 20℃ Of Stainless Steel 904L Seamless Heat Exchanger Tubes

Density g/cm3 Specific Heat Capacity J/kg K Thermal Conductivity
W/m K
Electrical Resistivity
Ωmm2/m
8.0 450 12 1

 

Customer Visit 

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

GNEE STEELGNEE STEEL

ASTM A249 904L SS Regenerative Heat Exchanger, Stainless Steel 904L  Heat Exchanger, UNS N08904 Precision Tube, DIN 1.4539 Bend Heat Exchanger Tube, SS 1.4539 Condenser Tubes Supplier in GNEE Steel, China.

 

Hot Tags: stainless steel 904l seamless heat exchanger tubes, China stainless steel 904l seamless heat exchanger tubes suppliers, 1 4509 1 4510 Pipes And Tubes, Slip On Flanges, 420J1 420J2 316 Stainless Pipe, Stainless Steel High Pressure Pipe, Inconel 625 Alloy Steel Plate, SS410 Stainless Steel Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry