Grade 630 17-4PH ASTM DIN EN Ss Pipe Seamless Length 3000mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of grade 630 17-4ph astm din en ss pipe seamless length 3000mm in China. If you're going to wholesale high quality grade 630 17-4ph astm din en ss pipe seamless length 3000mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Grade 630 17-4PH ASTM DIN EN Ss Pipe Seamless Length 3000mm
Description
| Application: | Construction,Decoration,Industry,Chemical | Standard: | DIN,ASTM |
|---|---|---|---|
| Steel Grade: | 304 304L 316 316L 310S 321 630.etc | Diameter: | 6 - 508mm |
| Type: | Seamless | Thickness: | 1-50mm |
| Length: | 3000mm~6000mm Or Cutting As Request | Shape: | Round.square.Rectangle |
| Service: | Cutting/ Polishing | ||
| High Light: |
EN 17-4PH Ss Pipe Seamless,Grade 630 Ss Pipe Seamless,Length 3000mm Ss Pipe Seamless |
||
Grade 630 Stainless Steel Seamless Pipe 17-4PH Stainless Steel pipe ASTM DIN EN SS Pipe
Detail informations of our 630 stainless steel pipe
| Name | Stainless Steel Pipe | Grade | 17-4PH / 630 |
| Type | Seamless Pipe | Diameter | DN 10 - DN300 |
| Thickness | SCH10 - XXS | Standard | ASTM GB JIS EN DIN |
| Length | 6m random length | Service | Cutting |
Grade Informations
17-4PH is a widely-used martensitic precipitation-hardening stainless steel with a high concentration of chromium and nickel. It has many favorable properties, including excellent strength, good corrosion resistance, and excellent mechanical properties up to 600 °F (316 °C).
The alloy also possesses good toughness when welded, while short low-temperature heat treatments reduce warping and scaling. Additionally, 17-4PH is easy to machine and fabricate.
Thanks to the beneficial properties, 17-4PH finds use in various industries. Typical parts include mechanical seals, oil patch, and pump shafts.
Furthermore, the alloy also finds use in the aerospace industry, petroleum industry, and chemical industry, food processing equipment, paper and pulp industry, nuclear waste processing and storage, and general metalworking.
Stainless Steel 17-4PH Chemical Composition
| Element | Min (%) | Max (%) |
| Carbon, C | – | 0.07 |
| Manganese, Mn | – | 1 |
| Silicon, Si | – | 1 |
| Sulfur, S | – | 0.03 |
| Phosphorus, P | – | 0.04 |
| Chromium, Cr | 15 | 17.5 |
| Niobium + Tantalum, Nb + Ta | 0.15 | 0.45 |
| Nickel, Ni | 3.0 | 5.0 |
| Copper, Cu | 3.0 | 5.0 |
| Iron, Fe | – | *Balance |
Stainless Steel 17-4PH Mechanical Properties
| Property | Imperial | Metric |
| Ultimate Tensile Strength | 23,300 psi | 160 MPa |
| Yield Strength (0.02%) | 16,680 psi | 115 MPa |
| Elongation (% in 2'') | 5% | 5% |
| Rockwell Hardness C | 35 | 35 |
Application of 17-4PH stainless steel
Jet engine stator vanes
Surgical instruments
Aerospace components
Components for the chemical, petrochemical and food processing industries
Products' Photos



Hot Tags: grade 630 17-4ph astm din en ss pipe seamless length 3000mm, China grade 630 17-4ph astm din en ss pipe seamless length 3000mm suppliers, SS410 Stainless Steel Pipe, 410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe, Slip On Flanges, 1 4509 1 4510 Pipes And Tubes, 420J1 420J2 316 Stainless Pipe