Black Carbon ERW Large Diameter Rectangular Tube En 10025 S355 100x200x6mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of black carbon erw large diameter rectangular tube en 10025 s355 100x200x6mm in China. If you're going to wholesale high quality black carbon erw large diameter rectangular tube en 10025 s355 100x200x6mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Black Carbon ERW Large Diameter Rectangular Tube En 10025 S355 100x200x6mm
Description
| Certification: | ISO9001-2000 | Alloy Or Not: | Non-alloy |
|---|---|---|---|
| Technique: | ERW | Thickness: | 2.87 - 13.84 Mm |
| Application: | Structure Pipe | Length: | 5.8-12m |
| Shape: | Square | ||
| High Light: |
en 10025 large diameter rectangular tube,100x200 large diameter rectangular tube,s355 carbon rectangular tube |
||
SS400 Black Welded Steel Square Tubing RHS 0.45 - 30 mm Wall Thickness
| SIZE: | 10x10-1200x1200mm |
| SIZE TORLERENCE: | +/-0.03mm |
| WALL THICKNESS: | 0.45-30mm |
| TORLERENCE: | +/-0.03mm |
| STANDARD: | GB/T 3094-2000 ASTM A 500 JIS G 3466 |
| CERTIFICATE: | ISO BV SGS |
| MATERIAL: | Q195 /Q215/Q235/ Q345 |
| TECHNIQUE: | Welded , cold-rolled. |
| SECTION SHAPE: | Rectangular |
| PACKING: |
1. In bundle with strip 2. By PP Woven material and anti-water plastic 3. As the customer's requirement. |
|
SURFACE TREATMENT: |
1)Black , Pre-galvanized 2)oiled , powder coating 3)Galvanized as your requirement |
| USAGE: |
Car-making ,machine manufacturing , Container Frame, Furniture |
| MAIN MARKET: | Middle East, Africa , North and South America , East and West Europe , Southeast Asia Australia |
| PAYMEN& SHIPPMENT TERMS: | |
| MINIMUM ORDER QUANTITY: | 25 metric tones |
| PORT: | SHANGHAI |
| DELIVERY TIME: | 20 days after receiving the LC or deposit |
| PAYMENT TERM: | LC at sight TT D/P ,ect |
| SUPPLY ABILITY: | 10000mts per month |
EN 10025 S355 Steel
S355 steel is a European standard structural steel grade, according to EN 10025-2: 2004, material S355 is divided into 4 main quality grades:
S355JR (1.0045),
S355J0 (1.0553),
S355J2 (1.0577) and
S355K2 (1.0596).
The properties of structural steel S355 is better than steel S235 and S275 in yield strength and tensile strength.
Steel Grade S355 Meaning (Designation)
The following letters and numbers explains the steel grade S355 meaning.
"S" is short for "structural steel"
"355" refers to the minumum yield strength value for the flat and long steel thickness ≤ 16mm.
"JR" means the impact energy value is minumum 27 J at room temperature (20℃).
"J0" can withstand the impact energy at least 27 J at 0℃.
"J2" related to the minumum impact energy value is 27 J at -20℃.
"K2" refers to the minumum impact energy value is 40 J at -20℃.
Datasheet and Specification
Below are the tables to show the steel grade S355 datasheet including chemical composition, yield strength, tensile strength and elongation, etc. All data sheet of DIN EN 10025-2 is the same as BS EN 10025-2 and other EU member states.
Chemical Composition
The datasheet below shows grade S355 steel chemical composition.
| S355 Chemical Composition % (≤) | ||||||||||
| Standard | Steel | Grade | C | Si | Mn | P | S | Cu | N | Method of deoxidation |
| EN 10025-2 | S355 | S355JR | 0.24 | 0.55 | 1.60 | 0.035 | 0.035 | 0.55 | 0.012 | Rimmed steel is not allowed |
| S355J0 (S355JO) | 0.20 | 0.55 | 1.60 | 0.030 | 0.030 | 0.55 | 0.012 | |||
| S355J2 | 0.20 | 0.55 | 1.60 | 0.025 | 0.025 | 0.55 | – | Fully killed | ||
| S355K2 | 0.20 | 0.55 | 1.60 | 0.025 | 0.025 | 0.55 | – | Fully killed | ||
Mechanical Properties
The datasheet below gives EN 10025 S355 steel mechanical properties such as yield strength, tensile strength and elongation.
Yield Strength
| S355 Yield Strength (≥ N/mm2); Dia. (d) mm | |||||||||
| Steel | Steel Grade (Steel Number) | d≤16 | 16< d ≤40 | 40< d ≤63 | 63< d ≤80 | 80< d ≤100 | 100< d ≤150 | 150< d ≤200 | 200< d ≤250 |
| S355 | S355JR (1.0045) | 355 | 345 | 335 | 325 | 315 | 295 | 285 | 275 |
| S355J0 (1.0553) | |||||||||
| S355J2 (1.0577) | |||||||||
| S355K2 (1.0596) | |||||||||
Tensile Strength
| S355 Tensile Strength (≥ N/mm2) | ||||
| Steel | Steel Grade | d<3 | 3 ≤ d ≤ 100 | 100 < d ≤ 250 |
| S355 | S355JR | 510-680 | 470-630 | 450-600 |
| S355J0 (S355JO) | ||||
| S355J2 | ||||
| S355K2 | ||||
Elongation
| Elongation (≥%); Thickness (d) mm | ||||||
| Steel | Steel Grade | 3≤d≤40 | 40< d ≤63 | 63< d ≤100 | 100< d ≤ 150 | 150< d ≤ 250 |
| S355 | S355JR | 22 | 21 | 20 | 18 | 17 |
| S355J0 (S355JO) | ||||||
| S355J2 | ||||||
| S355K2 | 20 | 19 | 18 | 18 | 17 | |



Hot Tags: black carbon erw large diameter rectangular tube en 10025 s355 100x200x6mm, China black carbon erw large diameter rectangular tube en 10025 s355 100x200x6mm suppliers, Slip On Flanges, 410 Stainless Steel Pipe, 1 4509 1 4510 Pipes And Tubes, 420J1 420J2 316 Stainless Pipe, SS410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe