ASTM A312 TP347H Stainless Steel Seamless Pipes
video

ASTM A312 TP347H Stainless Steel Seamless Pipes

Stainless Steel Seamless (SMLS) pipe is formed by drawing a solid billet over a piercing rod to create the hollow shell. As the manufacturing process does not include any welding, Seamless Pipes are perceived to be stronger and more reliable. Historically, seamless pipe was regarded as withstanding pressure better than other types, and was often more available than Welded Pipe.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a312 tp347h stainless steel seamless pipes in China. If you're going to wholesale high quality astm a312 tp347h stainless steel seamless pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM A312 Gr Tp347h ss pipe is an austenitic stainless steel tube. It has chromium and nickel content which give it the corrosion resistant properties. For extra toughness, the A312 347h material has higher carbon content. The addition of more carbon causes toughness but is also less strong than the low carbon version of the same material. But to overcome the issue, columbium is added in the A312 Tp347h material. The alloy composition makes the material resistant to most oxidizing agents. Regardless of the high carbon content, the SA 312 Tp 347h material has excellent resistance to intergranular corrosion. This makes the 347h Stainless Steel Pipe be applied in applications that operate under high temperatures with high risk of oxidization. The SS 347H Seamless Pipe material is cold drawn and therefore cannot be hardened by heat treatment. But it could be hardened by cold working. The material could also be easily welded upon.

ss pipesemaless pipe stainless

 

 

Chemical Composition of ASTM A312 TP347H Stainless Steel Seamless Pipes

 

Element 347 347H
Chromium 17.00 min.-19.00 max. 17.00 min.-19.00 max.
Nickel 9.00 min.-13.00 max. 9.00 min.-13.00 max.
Carbon 0.08 0.04 min.-0.10 max.
Manganese 2.00 2.00
Phosphorus 0.045 0.045
Sulfur 0.03 0.03
Silicon 0.75 0.75
Columbium & Tantalum 10 x (C + N) min.-1.00 max. 8 x (C + N) min.-1.00 max.
Iron Balance Balance


Mechanical Properties of ASTM A312 TP347H Stainless Steel Seamless Pipes

Yield Strength
0.2% Offset
Ultimate Tensile
Strength
Elongation
in 2 in.
Hardness
psi (min.) (MPa) psi (min.) (MPa) % (min.) (max.)
30,000 205 75,000 515 40 201 Brinell


ASTM A312 TP347H Stainless Steel Seamless Pipes Physical Properties

Properties Metric
Density 7.96 g/cm3


ASTM A312 TP347H Stainless Steel Seamless Pipes Application

  • Aerospace.
  • Laboratory benches & equipment.
  • Coastal architectural panelling, railings & trim.
  • Boat fittings.
  • Chemical Processing.
  • Heat Exchangers.
  • Woven or welded screens for mining, quarrying & water filtration.
  • Threaded fasteners.
  • Springs.

 

Customer Visit

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

gnee steelgnee steel

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: astm a312 tp347h stainless steel seamless pipes, China astm a312 tp347h stainless steel seamless pipes suppliers, 1 4509 1 4510 Pipes And Tubes, Inconel 625 Alloy Steel Plate, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe, Slip On Flanges, SS410 Stainless Steel Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry