2.4660 Stainless Steel Pipe And Tube
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 2.4660 stainless steel pipe and tube in China. If you're going to wholesale high quality 2.4660 stainless steel pipe and tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
2.4660 Stainless Steel Pipe and tube
2.4660 is widely used in the medical device industry, such as artificial joints, dental implants, surgical instruments, etc. 2.4660 is often used in food processing, chemical industry and other fields, because these fields have high requirements for the corrosion resistance and antibacterial properties of materials, and 2.4660 can meet these requirements.
2.4660 Typical chemical composition:
Carbon C: 0.07
Silicon Si: 1.0
ManganeseMn: 2.0
Phosphorus P: 0.045
Sulfur S: 0.035
Nickel: 32-38
Chromium Cr: 19-21
Molybdenum Mo: 2.0-3.0
Copper Cu: 3.0-4.0
Nb+Ta:1.0
Iron: balance

Hot Tags: 2.4660 stainless steel pipe and tube, China 2.4660 stainless steel pipe and tube suppliers, alloy seamless tubing, incoloy stainless pipe, , inconel alloy piping, , hastelloy ss piping