ASTM A312 TP310S Stainless Steel Seamless Pipes
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a312 tp310s stainless steel seamless pipes in China. If you're going to wholesale high quality astm a312 tp310s stainless steel seamless pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GNEE Steel offer ASTM A312 SS 310S Seamless Pipe is utilized for ease of fabrication.ASTM A312 TP310S Welded Pipe also known as UNS S31008 Pipes. SS 310S seamless pipe is quite resistance to hot corrosion. Stainless Steel 310S Seamless Pipes and SS 310S Welded Pipes has strength and toughness at cryogenic temperatures. As compare to comparison to carbon steel, these 310S Stainless Steel Pipes are tougher and tend to work harden rapidly.These TP310S ASTM A312 Stainless Steel Seamless Pipes has oxidation resistance to 2000°F.
Grade 310S (UNS S31008) is used when the application environment involves moist corrodents in a temperature range lower than that which is normally considered "high temperature" service. The lower carbon content of 310S does reduce its high temperature strength compared to 310.


ASTM A312 TP310S Seamless SS Pipes Physical Properties
| SUS | Tensile Strength minimum (MPa) | Yield Strength 0.2% Proof minimum (MPa) | Elongation minimum (% in 50mm) | Hardness | |
| Rockwell B (HR B) maximum | Brinell (HB) maximum | ||||
| 310S | 515 | 205 | 40 | 95 | 217 |
SA312 TP310s Chemical Material Composition
| ASTM A312 | Si | P | C | Mn | S | Cr | Mo | Ni | N | |
| 310s | min. | – | – | – | – | – | 24.0 | – | 19.0 | – |
| max. | 1.50 | 0.045 | 0.25 | 2.0 | 0.030 | 26.0 | 22.0 | – | ||
Equivalent Material of SA 312 AISI 310s
| GRADE | UNS | WERKSTOFF NR. | JIS | BS | EN | SS |
| USA | GERMAN | JAPAN | BRITISH | EUROPE | SWEDISH | |
| ASTM A312 310S | S31008 | 1.4845 | SUS 310S | - | - | - |
Customer Visit
GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.


Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.
Hot Tags: astm a312 tp310s stainless steel seamless pipes, China astm a312 tp310s stainless steel seamless pipes suppliers, 1 4509 1 4510 Pipes And Tubes, 410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, Stainless Steel High Pressure Pipe, SS410 Stainless Steel Pipe, Inconel 625 Alloy Steel Plate
You Might Also Like
Send Inquiry