Stainless Steel 316/316L/316Ti Pipes & Tubes
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 316/316l/316ti pipes & tubes in China. If you're going to wholesale high quality stainless steel 316/316l/316ti pipes & tubes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Pipes and tubes are commonly used in industrial application equipment. This is the way that the fluids or the liquids which are there in the industries. It is the reason that the industrial applications and the work is moving on smoothly. And the pipes and tubes are available in many shapes and sizes with which they are used in particular applications. Some of the types in which the pipes and tubes are available are round, square, rectangular, and others. It is the way that the applications are working with the best types of pipes and tubes available.
SS 316Ti is referred to as the stabilized grade alloy which is used in the alloying equipments. However, this is the alloy that is used with higher temperature situations applications. In addition to the other contents present in the alloy, the alloy type is having the high content of the titanium.
The alloying elements are the reason that the SS 316/316L/316Ti Pipes & Tubes are having different properties. Some of the properties which are there with the pipes and tubes are great toughness, ductility, durability, weldability, stability in the elevated temperatures, and others. This is the way that the pipes and tubes are used in the industrial applications.
316/316L/316TI STAINLESS STEEL PIPES AND TUBES EQUIVALENT GRADES
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST |
|---|---|---|---|---|---|---|---|
| SS 316 | S31600 | 1.4401 / 1.4436 | Z7CND17‐11‐02 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 | SUS 316 | 316S31 / 316S33 | - |
| SS 316L | S31603 | 1.4404 / 1.4435 | Z3CND17‐11‐02 / Z3CND18‐14‐03 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 | SUS 316L | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 |
| SS 316Ti | S31635 | 1.4571 | Z6CNDT17‐123 | X6CrNiMoTi17-12-2 | SUS 316Ti | 320S31 | 08Ch17N13M2T |
Stainless Steel 316/316L/316Ti Pipes and Tubes Other Types

SS 316/316L/316TI SEAMLESS PIPES
Stainless Steel 316 Seamless Pipes, UNS S31600/ S31603 / S31635 Seamless Pipes, DIN 1.4401 Seamless Pipes, ASME SA 312 SS TP316Ti Seamless Piping

SS 316/316L/316TI SEAMLESS TUBES
ASME SA213 SS 316L /316Ti Seamless Tube, ASTM A213 Stainless Steel 316 Seamless Tubing, DIN 1.4404 Seamless Tubes, UNS S31603 / S31635 Seamless Tube

SS 316/316L/316TI WELDED PIPES
Stainless Steel ASTM A312 TP316 Welded Pipes, UNS S31600/ DIN 1.4571 Welded Pipe, ASME SA312 SS 316L Welded Pipes, SS 316Ti Welded Pipe Supplier

SS 316/316L/316TI WELDED TUBES
DIN 1.4404 Welded Tubing, UNS S31600 Welded Tube, ASME SA 213 Stainless Steel 316L Welded Tubes, ASTM A213 316Ti SS Welded Tubes

SS 316/316L/316TI EFW PIPES
ASME SA358 316 SS EFW Pipes, ASTM A358 TP316Ti Stainless Steel EFW Pipe, SS UNS S31600/ S31603/ S31635 EFW Pipes, SS DIN 1.4404 / 1.4571 EFW Pipes

SS 316/316L/316TI ERW PIPES & TUBES
UNS S31600 ERW Pipes, Stainless Steel 316 ERW Tubing, ASTM A213 TP316L Stainless Steel ERW Tubes, ASME SA 312 SS 316Ti Pipe
Specification of Stainless Steel 316/316L/316Ti Seamless Welded Pipes And Tubes
CHEMICAL COMPOSITION OF STAINLESS STEEL 316/316L/316TI SEAMLESS PIPES AND TUBES
| Element | C | Mn | Si | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| 316 (S31600) |
0.08 max |
2.0 max |
0.75 max |
0.045 max |
0.03 max |
min: 16.0 max: 18.0 |
min: 2.0 max: 3.0 |
min: 10.0 max: 14.0 |
0.10 max |
| 316L (S31603) |
0.03 max |
2.0 max |
0.75 max |
0.045 max |
0.03 max |
min: 16.0 max: 18.0 |
min: 2.0 max: 3.0 |
min: 10.0 max: 14.0 |
0.10 max |
| 316TI(S31635) | - | - | - | - | - | 16.0 | 2.00 | 10.0 | - |
| 0.08 | 2 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.1 |
MECHANICAL PROPERTIES OF STAINLESS STEEL 316/316L/316TI SEAMLESS PIPES AND TUBES
| Grade | Tensile Strength ksi (min) |
Yield Strength 0.2% ksi (min) |
Elongation % | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 316 | 75 | 30 | 40 | 217 | 95 |
| 316L | 70 | 25 | 40 | 217 | 95 |
| 316TI | 515(Mpa) | 205(Mpa) | 35 | 205 | 75 |
PHYSICAL PROPERTIES OF 316/316L/316TI STAINLESS STEEL PIPES AND TUBES
| Density lbm/in3 |
Thermal Conductivity (BTU/h ft. °F) |
Electrical Resistivity (in x 10-6) |
Modulus of Elasticity (psi x 106 |
Coefficient of Thermal Expansion (in/in)/°F x 10-6 |
Specific Heat (BTU/lb/°F) |
Melting Range (°F) |
|---|---|---|---|---|---|---|
| 0.29 at 68°F | 100.8 at 68 212°F | 29.1 at 68°F | 29 | 8.9 at 32 – 212°F | 0.108 at 68°F | 2500 to 2550 |
| 9.7 at 32 – 1000°F | 0.116 at 200°F | |||||
| 11.1 at 32 – 1500°F |
,