Cold Rolled Steel Strip Black Annealing Coil DC01 SPCC Thickness 0.5-3.0mm 1250mm Width
video

Cold Rolled Steel Strip Black Annealing Coil DC01 SPCC Thickness 0.5-3.0mm 1250mm Width

Deep Drawing quality 1 Thickness: 0.3-2.0mm 2 Width: 700-1250mm 3 Inner diameter: 508mm 4 Steel Grade: SPCD, SPCE, DC03 5 Packing: standard export packing 6 Cutting and slitting can be requested as customer's designation.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of cold rolled steel strip black annealing coil dc01 spcc thickness 0.5-3.0mm 1250mm width in China. If you're going to wholesale high quality cold rolled steel strip black annealing coil dc01 spcc thickness 0.5-3.0mm 1250mm width made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Cold Rolled Steel Strip Black Annealing Coil DC01 SPCC Thickness 0.5-3.0mm 1250mm Width

Description

Thickness: 0.5-3.0MM Width: 10-1500mm
Surface: Black ,Bright Type: Cold Rolled
High Light:

low carbon steel plate

,

high carbon steel plate

Cold rolled steel sheet in coil

Deep Drawing quality

1 Thickness: 0.3-2.0mm

2 Width: 700-1250mm

3 Inner diameter: 508mm

4 Steel Grade: SPCD, SPCE, DC03

5 Packing: standard export packing

6 Cutting and slitting can be requested as customer's designation.

COLD ROLLED STEEL COILS(CRC)
Width (mill edge): 914-1500mm
Max. Thickness: 0.3--2.0mm
Min. Thickness: 0.3mm
Inside diameter: 508mm or 610mm
Outside diameter: 850~1500mm
Description of goods: we can supply soft, semi-soft, cold hard and stainless worked cold-rolled steel coils at customer's option
Steel Grade: SPCC-SD, SPCC-1B, DC01, DC02, DC03, DC04

 

Name Cold rolled steel coil/sheet
Standard JIS 3302 / ASTM A653 / EN10143
Grade Q235, SGCC, CGCC, SPCC, DX51D, DX52D, SPHC, DC01, DC03, DC04, ST12
Width 750~1250mm
Thickness 0.12~3.0mm
Surface treatment chromated / galvanized/oiled/annealed
ID coil 508mm or 610mm
Coil weight 3-8 MT
Package: Standard exporting package
Application Industrial panels, roofing and siding for painting
Price terms FOB,CFR,CIF
Payment terms 30%TT in advance+70% TT or irrevocable 100%L/C at sight
delivery time within 25 days

 

Cold Rolled Steel Strip Black Annealing Coil DC01 SPCC Thickness 0.5-3.0mm 1250mm Width 0Cold Rolled Steel Strip Black Annealing Coil DC01 SPCC Thickness 0.5-3.0mm 1250mm Width 1

Hot Tags: cold rolled steel strip black annealing coil dc01 spcc thickness 0.5-3.0mm 1250mm width, China cold rolled steel strip black annealing coil dc01 spcc thickness 0.5-3.0mm 1250mm width suppliers, 304 316 316l SS Cold Rolled Steel Coils, 2507 Stainless Steel Coil, AISI430 Stainless Steel Foil, 316L Stainless Steel Coil