Full Hard UNS S30100 301 Stainless Steel Coils No Magnetic 2000mm Width
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of full hard uns s30100 301 stainless steel coils no magnetic 2000mm width in China. If you're going to wholesale high quality full hard uns s30100 301 stainless steel coils no magnetic 2000mm width made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
301 Stainless Steel Full Hard UNS S30100 301 Stainless Steel Strip No Magnetic
301-1/2 Hard is an austenitic stainless steel that it has been cold rolled to its 1/2 hard condition. This makes it ideal for applications requiring both formability and tensile strength of 150,000 PSI and yield strength of 110,000 PSI.
Standard Inventory Specifications
UNS S30100
AMS 5518
ASTM A 666
ASTM SA 666
EN 1.4310
PWA-LCS
GE-S400/1000
RR SABRe Edition 2
DFARS Compliant
Common Applications of 301-1/2 Hard Stainless Steel
Aircraft structural parts
Trailer bodies
Architectural (roof drainage/door frames, etc.)
Auto body trim and wheel covers
Utensils and tablewear
Conveyor parts
Inventory Size Range
Sheet : 0.009" - 0.130"
Please contact us for more details.
The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.
301-1/2 Hard Chemical Composition
| Element | Percent by Weight |
|---|---|
| Carbon | 0.15 maximum |
| Manganese | 2.00 maximum |
| Phosphorus | 0.045 maximum |
| Sulfur | 0.03 maximum |
| Silicon | 1.00 maximum |
| Chromium | 16.00 - 18.00 |
| Nickel | 6.00 - 8.00 |
| Nitrogen | 0.10 maximum |
301-1/2 Hard Stainless Steel Physical Properties
Melting Range: 2250-2950°F (1399-1421°C)
Density: 0.2850 lb/in3 (7.88 g/cm3)
Specific Gravity: 8.03
Modulus of Elasticity in Tension: 28 x 106 psi (193 GPa)*
* In the cold worked condition, the modulus is lowered.
| Temperature Range | Coefficients | ||
|---|---|---|---|
| °C | °F | cm/cm°C | in/in/°F |
| 20-100 | 68-212 | 16.6 x 10-6 | 9.2 x 10-6 |
| 20-300 | 68-572 | 17.6 x 10-6 | 9.8 x 10-6 |
| 20-500 | 68-932 | 18.6 x 10-6 | 10.3 x 10-6 |
| 20-700 | 68-1292 | 19.5 x 10-6 | 10.8 x 10-6 |
| 20-871 | 68-1600 | 19.8 x 10-6 | 11.0 x 10-6 |
| Temperature Range | Coefficients | ||
|---|---|---|---|
| °C | °F | W/m·K | Btu/(hr/ft²/in/°F) |
| 20-100 | 68-212 | 16.3 | 9.4 |
| 20-500 | 68-932 | 21.4 | 12.4 |
| Temperature Range | J/kg°K | Btu/lb/°F | |
|---|---|---|---|
| °C | °F | ||
| 0-100 | 32-212 | 500 | 0.12 |
Magnetic Permeability
H/m Annealed 1.02 Max @ 200 H
| Temperature Range | microhm-cm | microhm-in | |
|---|---|---|---|
| °C | °F | ||
| 20 | 68 | 72 | 28.3 |
| 100 | 212 | 78 | 30.7 |
| 200 | 392 | 86 | 33.8 |
| 400 | 752 | 100 | 39.4 |
| 600 | 1112 | 111 | 43.7 |
| 800 | 1472 | 121 | 47.6 |
| 900 | 1652 | 126 | 49.6 |
Mechanical Properties and Yield Strength of 301-1/2 Hard
| Condition | Tensile Strength, Min. | 0.2% Yield Strength, Min. | Elong. In 2" (50mm) | ||
|---|---|---|---|---|---|
| Ksi | MPa | Ksi | MPa | %, Min. | |
| Annealed | 75 | 515 | 30 | 205 | 40 |
| 1/4 Hard | 125 | 862 | 75 | 517 | 25 |
| 1/2 Hard | 150 | 1034 | 110 | 758 | 18* |
| 3/4 Hard | 175 | 1207 | 135 | 931 | 12* |
| Full Hard | 185 | 1276 | 140 | 965 | 9* |
* Value shown for thickness greater than 0.015 in. (.038mm).

Hot Tags: full hard uns s30100 301 stainless steel coils no magnetic 2000mm width, China full hard uns s30100 301 stainless steel coils no magnetic 2000mm width suppliers, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil, AISI430 Stainless Steel Foil, 2507 Stainless Steel Coil