Stainless Steel 304L Cold Rolled Coils
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 304l cold rolled coils in China. If you're going to wholesale high quality stainless steel 304l cold rolled coils made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 304 Cold Rolled Coils and Stainless Steel 304L Cold Rolled Coils are a versatile material widely used for applications requiring good mechanical properties and excellent corrosion resistance. They offer outstanding workability, formability, durability, and weldability and can be easily machined.

Stainless Steel 304L Cold Rolled Coils have low carbon content that allows them to be easily deep-drawn without any annealing process required. They also provide excellent resistance to stress cracking corrosion (SCC) compared to conventional stainless steels. Additionally, they offer higher tensile strength than other austenitic stainless steel grades such as 316 or 316L in cold rolled condition.
|
Material |
Specification |
Standards |
Size |
Length |
|
Stainless Steel Coils
|
ASTM, ASME and API |
ASTM A 240 / ASME SA 240 |
M02 to M30 |
3 mm To 200 mm |

These Stainless Steel 304 CR Coils are ideal for use in structural components and pressure vessels, storage tanks, automotive components, kitchen and bathroom accessories, medical equipment, construction projects, and oil & gas industries. They are also used in the manufacture of consumer products such as cutlery, cooking utensils, sinks, and furniture.
Stainless Steel 304L CR Coils have excellent formability that allows for easy bending or roll forming without losing strength or ductility. Additionally, they offer good ductility which gives them better machinability compared to other grades of stainless steel cold-rolled coils.
Hot Tags: stainless steel 304l cold rolled coils, China stainless steel 304l cold rolled coils suppliers, 2507 Stainless Steel Coil, AISI430 Stainless Steel Foil, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil