ASTM A240 S32205 Stainless Steel Coil Cold Rolled 2205 Duplex Steel Strip Coil S31803
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a240 s32205 stainless steel coil cold rolled 2205 duplex steel strip coil s31803 in China. If you're going to wholesale high quality astm a240 s32205 stainless steel coil cold rolled 2205 duplex steel strip coil s31803 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Part 1. Stainless steel coil desription
|
Product type |
ASTM A240 S32205 Stainless Steel Coil |
|
|
Thickness |
0.3mm-45mm |
|
|
Diameter |
30mm-560mm |
|
|
Quantity |
as customer's requirement |
|
|
Finish |
2B,BA,HL,MIRROR,NO.1-NO.4,8K,and so on. |
|
|
Standard |
ASME, ASTM, EN ,BS,GB,DIN, JIS etc |
|
|
Material |
2205, 201, 202, 301, 304, 410, 430, 409 |
|
|
Application range |
Foodstuff, Gas, metallurgy, biology, electron, chemical, petroleum, |
|
|
Package |
Standard export sea-worthy packing |
|
|
Delivery time |
5-8 days |
|
|
Quality |
No.1 |
|
|
Productivity |
3000-4000 tons/month |
|
|
Contact us |
Person |
Gao Ben |
|
Mobile |
+86-18068357371 |
|
|
|
+86-18068357371 |
|
|
|
wxgms |
|
|
Skype |
benwallace2012 |
|
|
|
1461733389 |
|
Part 2. Surface & Application
|
Surface |
Application |
|
2B |
Medical equipment, Food industry, Construction material, Kitchen utensils |
|
BA |
Kitchen utensils, Electric equipment, Building construction |
|
No.1 |
Chemical tank, pipe |
|
No.4 |
Kitchen utensils, Building construction, Medical equipment |
|
HL |
Building construction |





Part 3. Chemical composition
|
Material |
C |
Si |
Mn |
P |
S |
Cr |
Ni |
|
201 |
≤0.12 |
≤0.75 |
9.5-12.5 |
≤0.045 |
≤0.03 |
13-16 |
0.8-1.5 |
|
304 |
≤0.08 |
≤0.75 |
≤2.0 |
≤0.045 |
≤0.03 |
18-19 |
8-10 |
|
316 |
≤0.08 |
≤1.00 |
≤2.0 |
≤0.035 |
≤0.03 |
10-14 |
16.0-18.5 |
|
316L |
≤0.03 |
≤1.0 |
≤2.0 |
≤0.035 |
≤0.03 |
16-18 |
10-14 |
|
430 |
≤0.12 |
≤0.75 |
≤2.0 |
≤0.04 |
≤0.03 |
16-18 |
≤0.6 |

Hot Tags: astm a240 s32205 stainless steel coil cold rolled 2205 duplex steel strip coil s31803, China astm a240 s32205 stainless steel coil cold rolled 2205 duplex steel strip coil s31803 suppliers, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil, 2507 Stainless Steel Coil, AISI430 Stainless Steel Foil