What material is Inconel?
Inconel is a heat-resistant and corrosion-resistant nickel-chromium-iron alloy, a nickel-based alloy material.
Inconel600, Inconel601, Inconel625, Inconel718, Inconel617,, Inconel622,, Inconel 671,, Inconel672, Inconel686, Inconel690, Inconel693, Inconel706,, Inconel725, Inconel X-750, Inconel 751, Inconel754, Inconel7 58, Inconel783 and so on.
Inconel625
Overview of Incone l625 features and application areas:
This alloy is a solid solution strengthened nickel-based deformed high-temperature alloy with molybdenum and niobium as the main strengthening elements. It has excellent corrosion resistance and high oxidation properties, good tensile properties and fatigue properties from low temperature to 980°C, and is salt resistant. Stress corrosion in fog atmosphere. Therefore, it can be widely used in manufacturing aerospace engine parts, aerospace structural components and chemical equipment.
INCONEL600 is a nickel-chromium-iron-based solid solution strengthened alloy with good high-temperature corrosion resistance (acid and alkali resistance) and oxidation resistance, excellent hot and cold processing and welding process performance, and satisfactory thermal strength below 700°C. and high plasticity.
This alloy is designed for low temperature to 1093°C environments. It has extremely excellent oxidation resistance at high temperatures, and has good oxidation resistance and carbonization resistance stability at 1093°C (but in a reducing atmosphere containing hydrogen sulfide, its upper limit temperature is 535°C).
It is very effective in treating hydrogen chloride and chlorine gas at high temperatures; hydrogen chloride can reach about 538℃, and chlorine gas can be used safely up to 510℃. This alloy also has excellent corrosion resistance against nitrogen, hydrogen and carburizing, so it is used in various heat treatment furnaces.


Inconel601 (UNS N06601) nickel-based alloy
Inconel 601, an alloy material. Excellent oxidation resistance at high temperatures, good resistance to carbonization, good resistance to oxidation in sulfur-containing atmospheres, good mechanical properties at both room temperature and high temperature, good resistance to stress corrosion cracking due to controlled Due to the carbon content and grain size, 601 has higher creep rupture strength, so it is recommended to use 601 in areas above 500°C.
Features
1. Excellent oxidation resistance at high temperatures
2. Excellent carbonation resistance
3. Good resistance to oxidation in sulfur-containing atmospheres
4. It has good mechanical properties at both room temperature and high temperature.
5. Excellent resistance to stress corrosion cracking. Due to the control of carbon content and grain size, 601 has high creep rupture strength, so it is recommended to use 601 in areas above 500°C.
Metallographic structure of Inconel 601:
601 is a face-centered cubic lattice structure.
Corrosion resistance of Inconel 601:
An important property of 601 alloy is its oxidation resistance at temperatures up to 1180°C. Even under very severe conditions, such as during heating and cooling cycles, 601 can form a dense oxide film and achieve high peeling resistance. 601 has good carbonation resistance. Due to its high chromium and aluminum content, 601 has good oxidation resistance in high-temperature sulfur-containing atmospheres .
application
1. Trays, baskets and fixtures used in heat treatment factories.
2. Wire strand annealing and radiant tubes, high speed gas burners, wire mesh belts in industrial furnaces.
3. Isolation tanks in ammonia reforming and catalytic support grids in nitric acid manufacturing.
4. Exhaust system components
5. Combustion chamber of solid waste incinerator
6. Pipe supports and soot disposal components
7. Exhaust gas detoxification system components
8.Oxygen reheater