What material is GH706?

 

GH2706 (GH706) precipitation hardening deformed high temperature alloy/Inconel 706

GH2706 is a Fe-Ni-Cr-based precipitation hardening deformed high-temperature alloy with a service temperature below 550℃-650℃. This alloy is a modified alloy of GH4169 alloy and its characteristics are similar to GH4169 alloy. Due to the reduction of niobium content in the alloy, it has better production process performance, hot and cold processing performance and welding performance. The alloy has high strength, good oxidation resistance and corrosion resistance below 700°C. This alloy can produce large and super-large high-temperature alloy products, and is suitable for making parts such as aero-engine casings, diffuser casings, turbine disks, and fasteners. It can also be used to make large-diameter rings suitable for gas turbines for cycle power generation. pieces. The main products include bars, forgings, rings, sheets and strips, etc.

What material is GH706?

What material is GH706?

The alloy has been used to manufacture components such as engine high-pressure compressor extension casings.

The alloy has a wide hot working temperature range and has high plasticity in the range of 850℃-1150℃. When the deformation rate is 0.01, it quickly enters the steady-state rheology stage at 900℃-1100℃, and then the true stress changes very little, which is extremely beneficial for blanking and hot processing of large shapes. In the three-stage heat treatment of the alloy, 843°C*3h is the stabilization treatment. After the treatment, there is a large amount of eta phase on the grain boundaries. The existence of eta phase is conducive to the improvement of durable performance.

Heat treatment system

Hot rolled bars, forged bars, forgings: 925-980℃, water cooling + 845℃ insulation for 3 hours + 720℃ insulation for 8 hours, cooling at 55℃ per hour to 620℃, insulation for 8 hours, safe cooling. HBS>285

Density: 8.06
​

Send Inquiry