Mar 07, 2025 Leave a message

What Is The Difference Between INCONEL 750 And 718?

What is the difference between INCONEL 750 and 718?

 

 

What Is Inconel 718?
Inconel 718 Bar, 718 Inconel Alloy Bar
Inconel 718 is a nickel-based superalloy known for its high strength, corrosion resistance, and excellent weldability. It is precipitation-hardenable, meaning its mechanical properties can be enhanced through heat treatment.

Temperature Range: Performs well in temperatures ranging from -250°C to 700°C.
Corrosion Resistance: Outstanding resistance to oxidation, pitting, and stress-corrosion cracking, even in harsh environments.
Mechanical Strength: High tensile and yield strength due to its niobium content.
Applications: Commonly used in aerospace turbines, gas turbines, nuclear reactors, and oil and gas extraction.

What Is Inconel X-750?
Inconel X-750 is another nickel-based alloy that excels in high-temperature environments. It is also precipitation-hardenable but contains more aluminum and titanium than Inconel 718, contributing to its strength at elevated temperatures.

Temperature Range: Performs optimally at temperatures up to 980°C.
Creep Resistance: Superior resistance to deformation under long-term high-temperature stress.
Corrosion Resistance: Good resistance to oxidation and chemical corrosion, though slightly less than Inconel 718.
Applications: Frequently used in jet engines, nuclear reactors, springs, and fasteners.

inconel 718 material pipeinconel 718 special metals tubing

Inconel 718 vs Inconel X-750: What Are Their Differences?

Chemical Composition: Inconel 718 vs Inconel X-750

Both alloys share a nickel-chromium base but differ in secondary elements that define their performance characteristics:

Element Inconel 718 Inconel X-750
Ni 50-55% 70% minimum
Cr 17-21% 14-17%
Fe Bal. 5-9%
Mo 2.8-3.3% –
Ti 0.65-1.15% 2.25-2.75%
Al 0.2-0.8% 0.4-1%
Nb 4.75-5.5% –
Co 1% max 1% max

 

Mechanical Properties: Inconel 718 vs Inconel X-750

Property Inconel 718 Inconel X-750
Tensile Strength 1370 MPa 1100 MPa
Yield Strength 1030 MPa 780 MPa
Elongation 12-15% 15-20%
Hardness (Rockwell) B95-C36 B88-C32

 

 

Corrosion Resistance: Inconel 718 vs. Inconel X-750
Both alloys offer excellent corrosion resistance:

Inconel 718 resists pitting, crevice corrosion, and stress corrosion cracking more effectively, especially in aqueous and sour environments. It is the preferred choice for offshore oil and gas applications.
Inconel X-750 has excellent oxidation resistance at elevated temperatures, but its resistance to chemical attack is inferior to that of Inconel 718.

Performance in High Temperature Environments
Inconel 718:
Inconel 718 is designed for medium- and high-temperature applications, but begins to lose mechanical properties above 700°C. Its weldability makes it suitable for fabrication that requires precision.

Inconel X-750:
Inconel X-750 can withstand temperatures up to 980°C and has excellent creep resistance. This makes it more suitable for use in components such as turbine blades and nuclear reactor springs that are exposed to extreme temperatures for extended periods of time.

Applications of Inconel 718 and Inconel X-750
Benefits of Inconel 718
Excellent mechanical strength.
Better weldability.
Excellent resistance to pitting and stress corrosion cracking.
Benefits of Inconel X-750
Better high temperature performance.
Excellent creep resistance.
Ideal for applications exposed to high temperatures for long periods of time.

Cost of Inconel 718 and Inconel X-750
Inconel 718 tends to be more expensive because it contains higher levels of niobium and molybdenum, which improves its strength and corrosion resistance. Additionally, its superior performance in harsh and corrosive environments has increased demand, especially in industries such as oil and gas, aerospace, and offshore engineering.

Inconel X-750 is generally more affordable than Inconel 718. This is because it contains lower levels of expensive elements (such as molybdenum) and relies more on aluminum and titanium for precipitation hardening. Its lower production cost makes it a preferred choice for high temperature applications where corrosion resistance is less important.