What Is The Difference Between Incoloy 825 And Inconel 625?

 

What is Incoloy 825 material?

INCOLOY 825 alloy (UNS N08825/W.Nr. 2.4858) is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium. The chemical composition of the alloy is designed to provide excellent resistance to a wide range of corrosive environments.

What is the ASTM standard for Inconel 825?

ASTM B423 UNS N08825 Alloy 825 Welded Pipe and Cold Drawn Annealed Incoloy 825 Pipe Suppliers. Incoloy 825 is one of the most effective alloy choices for harsh environments. It performs well in a variety of climates, especially in terms of general and localized corrosion, which makes Incoloy WERKSTOFF NR the best choice.

What is the difference between Inconel 625 and Inconel 825

What is the difference between Inconel 625 and incoloy 825?

Inconel 625 is often used in sour gas service due to its good resistance to stress corrosion cracking and pitting, while incoloy 825 is often used in crude oil service due to its good corrosion resistance in sour environments.

What is Inconel 625 used for?

Some applications require the strength and corrosion resistance of INCONEL 625 alloy, such as bubble caps, piping, reaction vessels, distillation columns, heat exchangers, transfer piping and valves.

Difference-Between-Inconel-625-and-825-Comparison-Summary

 

  Alloy 825 Alloy 625
Material nickel-iron-chromium alloy 825 nickel-chromium alloy 625
Equivalent W.Nr. 2.4858
UNS N08825
W.Nr. 2.4856
UNS N06625
Density 0.294 lb/cu in 0.305 lb/cu in
Melting Range 1370-1400°C 1290-1350°C
Curie Temperature <-196°C -196°C
Thermal Conductivity 76.8 Btu • in/ft2•h•°F
11.1 W/m •°C.
68 Btu • in/ft2•h•°F
9.8 W/m •°C.

Alloy 825 vs Alloy 625 Applications and Uses

Inconel Alloy 625

Engine Exhaust Systems

Sea-water Applications

Aircraft Ducting Systems

Thrust-reverser Systems

Distillation Columns

Heat-exchanger And Boilers

Seals

Springs

Bellows

Incoloy Alloy 825

Chemical Processing

Acid Production

Nuclear Fuel Reprocessing

Oil And Gas Recovery

Pickling Operations

Difference between Inconel 625 and Incoloy 825

  Inconel 625 Incoloy 825
Defination It is nickel based superalloy which contains a high amount of nickel than any other grade of Inconel It is nickel based superalloy which contains a moderate amount of nickel as compared to any other grade of Inconel
Nickel Content It contains about 58% of nickel It contains about 36-48% of nickel
Tensile Strength It has very high tensile strength and yield strength It has comparatively low tensile strength and yield strength
Elongation It's elongation is about 42.52% It's elongation is about 30%