Incoloy 825
Approximate grades: UNS N08825, NCF825
Certification: ISO9001:2015
Alloy category: Corrosion-resistant alloy
Substrate shape: Axis wire/strip/straight bar
Alloy series: Nickel-chromium-iron alloy
Implementation standard: ASTM B564
Application areas: Marine ships, petrochemicals, energy fields
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of Incoloy 825 in China. If you're going to wholesale high quality Incoloy 825 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy 825, also known as Alloy 825, N08825 and W.Nr. 2.4858, is a nickel-iron-chromium alloy that contains molybdenum, copper and titanium. The alloy excels in resisting a wide range of corrosive environments, including those containing sulfuric and phosphoric acids as well as seawater and other chloride-containing environments.
Incoloy 825 is extremely resistant to reducing and oxidizing acids, stress corrosion cracking, and pitting and crevice corrosion. It is often used in applications such as chemical processing, pollution control, oil and gas recovery, pickling operations and offshore engineering. In addition, it is suitable for use in sulfuric and phosphoric acid processing equipment.
Standard product forms of INCOLOY 825 include tube, pipe, plate, strip, plate, round bar, flat bar, forgings, hexagonal bar and wire.
Incoloy 825 Specification
Chemical composition
|
C |
Al |
Si |
S |
Ti |
Cr |
Mn |
Fe |
Ni |
Cu |
Mo |
|
0.05 max |
0.2 max |
0.5 max |
0.03 max |
0.6 - 1.2 |
19.5 - 23.5 |
1.0 max |
22.0 min |
38.0 - 46.0 |
1.5 - 3.0 |
2.5 - 3.5 |
Mechanical properties
|
Tensile Strength (ksi) |
0.2% Yield Strength (ksi) |
Elongation% in 2 inches |
|
85 |
35 |
30 |
Physical properties
|
|
Units |
Temperature in°C |
|
Density |
8.14 g/cm³ |
Room |
|
Specific Heat |
0.105 Kcal/kg.C |
Room |
|
Melting Range |
1370 - 1400 °C |
- |
|
Modulus of Elasticity |
196 KN/mm² |
20° |
|
Electrical Resistivity |
113 µΩ.cm |
25° |
|
Coefficient of Expansion |
14.1µm/m °C |
25 - 100° |
|
Thermal Conductivity |
11.1 W/m -°K |
25° |
Nickel Alloy 825 Products Display
Incoloy® 825 Nickel Alloys

Why choosing GNEE
GNEE has invested in and built production lines for cold-rolled plates and stainless steel in China. At the same time, the company has established long-term and good cooperative relations with major domestic and international steel mills such as Baosteel, TISCO, and Posco, providing customers with high-quality products and services more conveniently and efficiently. In addition, the company has also set up several large warehouses in major domestic ports to ensure that the goods are delivered to customers as soon as possible.
please contact us in time to get a quote!ss@gneesteel.com
PRODUCTS TESTING

Alloy 800 Plate Supplier

ASTM B 409 N08800 Plate Stockists

FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: Incoloy 825, China Incoloy 825 suppliers, alloy forgings, alloy for microscopy baths, alloy for electrolyzers, Inconel Alloy 617 Seamless Pipe, alloy for filtration baths, alloy products
Previous
Incoloy 800Next
Incoloy 800HTYou Might Also Like
Send Inquiry