Inconel 625 VS Inconel 825

What are the benefits of Inconel 625 Alloy?
INCONEL 625 alloy has the following properties that make it ideal for seawater applications: low susceptibility to localized corrosion (pitting and crevice corrosion), high corrosion fatigue strength, high tensile strength, and resistance to chloride ion stress corrosion cracking.
What is the difference between Inconel 625 and Inconel 825?
The main difference between the two is that Inconel 625 has a higher nickel content than Incoloy 825. What is Inconel 625? Inconel 625 has a higher nickel content than other grades of Inconel and is a nickel-based high-temperature alloy. At high temperatures, it has high strength and high resistivity.


What is the difference between Inconel 625 alloy and Incoloy 800?
Inconel 625 alloy has high corrosion fatigue strength, tensile strength and resistance to chloride ion stress corrosion cracking. The advantage of Incoloy 800 alloy is that it is more resistant to various corrosion.
What is the difference between Inconel 625 and Monel 400?
The difference is that Monel 400 lacks very effective solid solution strengthening elements, so its strength is relatively limited. Inconel 625 adds two very effective solid solution strengthening elements, molybdenum and niobium, to obtain higher strength.

What is the difference between Inconel 625 and Inconel 825?
Inconel is a nickel-based superalloy. Inconel can be classified into different grades depending on the nickel content in the alloy and considering many other parameters. Inconel 625 and Incoloy 825 are two different grades. The main difference between the two is that Inconel 625 has a higher nickel content than Incoloy 825.
What is Inconel 625?
Inconel 625 has a higher nickel content than other grades of Inconel and is a nickel-based superalloy. At high temperatures, it has high strength and high resistivity. It has excellent protection against corrosion and oxidation. These unique advantages make it very useful in nuclear and marine applications.
Inconel 625 alloy has a service temperature range from cryogenic to 982°C. The alloy's high strength is derived from the strengthening effect of niobium and molybdenum in a nickel-chromium matrix. Therefore, precipitation hardening is not required for Inconel alloy. Inconel 625 alloy has high tensile strength, high corrosion fatigue strength, and resistance to chloride ion stress corrosion cracking, making it an ideal choice for seawater applications. In addition, it exhibits excellent toughness and ductility at cryogenic temperatures.
Inconel Alloy 625 Chemical Composition
| Inconel | Element (% by mass) | ||||||||||||||
| Ni | Cr | Fe | Mo | Nb | Co | Mn | Cu | Al | Ti | Si | C | S | P | B | |
| 625 | 58.0 | 20.0–23.0 | 5.0 | 8.0–10.0 | 3.15–4.15 | 1.0 | 0.5 | 0.4 | 0.4 | 0.5 | 0.1 | 0.015 | 0.015 | ||
Inconel 625 Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation | |
| 625 | 8.4 g/cm3 | 1350 °C (2460 °F) | Psi – 135,000 , MPa – 930 | Psi – 75,000 , MPa – 517 | 42.5 % |
What is Incoloy 825?
When compared to other Inconel grades, Incoloy 825 contains a moderate amount of nickel and is a nickel based superalloy. It consist a higher melting point but has low yield strength and a low tensile strength. And it contains chromium and nickel along with titanium, molybdenum and copper. It specifically provides an exceptional corrosion resistance to aqueous corrosion. Beside this, it exhibits oxidizing resistance and reducing acids such as phosphoric and sulfuric acids.
Incoloy 825 Material Composition
| Alloy | Ni | Cr | Fe | Mb | Ti | Cu | Mn | C | S | Al | Si |
| Incoloy 825 | 38.0 – 46.0 | 19.5 – 23.5 | 22.0 min | 2.5 – 3.5 | 0.6 – 1.2 | 1.5 – 3.0 | 1.0 max | 0.05 max | 0.03 max | 0.2 max | 0.5 max |
Alloy 825 Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.14 g/cm3 | 1400 °C (2550 °F) | Psi – 80,000 , MPa – 550 | Psi – 32,000 , MPa – 220 | 30 % |
Difference between Inconel 625 and Incoloy 825
| Inconel 625 | Incoloy 825 | |
| Defination | It is nickel based superalloy which contains a high amount of nickel than any other grade of Inconel | It is nickel based superalloy which contains a moderate amount of nickel as compared to any other grade of Inconel |
| Nickel Content | It contains about 58% of nickel | It contains about 36-48% of nickel |
| Tensile Strength | It has very high tensile strength and yield strength | It has comparatively low tensile strength and yield strength |
| Elongation | It's elongation is about 42.52% | It's elongation is about 30% |