Inconel 625 VS 718 Alloy

Can INCONEL Alloy 718 be Cold Worked?
This alloy is cold worked after solution annealing and is typically used to make high-strength fasteners requiring a minimum room temperature tensile strength of 220 ksi, which can be achieved after precipitation hardening. This alloy is typically used at temperatures up to 900°F. This grade resists oxidation up to 1800°F.
What is the difference between Inconel 625 and Inconel 718?
Inconel 625 and Inconel 718 share many of the properties of the Inconel family. But the key difference between them is that the main property of Inconel 625 is high corrosion resistance, while the main property of Inconel 718 is high strength. Both alloys have their uses and cannot replace each other.


What does UNS N07718 correspond to?
Inconel Alloy 718 (corresponding to Inconel 718) - American Standard UNS N07718.
What is Inconel 718 used for?
It is also used to make components, rings and casings for liquid-fuel rockets, as well as various formed sheet metal parts for aircraft and land-based turbine engines. In extreme temperature conditions, INCONEL 718 alloy is also used for cryogenic storage tanks.

Inconel 625 and 718 specifications
Specifications of inconel 625 vs inconel 718
| Specification | Inconel 718 | Inconel 625 |
| Tensile Strength | 135 ksi (930 MPa) | 135 ksi (930 MPa) |
| Melting Point | 2300°F (1260°C) | 2350°F (1290°C) |
| Density | 8.19 g/cm³ | 8.44 g/cm³ |
| Yield Strength | 95 ksi (655 MPa) | 75 ksi (517 MPa) |
Inconel 625 vs 718: Chemical Composition
There are several factors to consider when choosing between Inconel 625 and Inconel 718 for your project. Inconel 625 is primarily composed of nickel and chromium, while Inconel 718 contains nickel, chromium, niobium, and molybdenum. Each alloy has its own strengths and is suitable for different applications.
Inconel 625 is suitable for sour environments, but may require additional protection in some cases. Inconel 718, by contrast, is more protective and easier to weld. The final choice depends on your specific needs, so it is important to understand their characteristics before making a decision.
| Element | Inconel 625 Composition (%) | Inconel 718 Composition (%) |
| Nickel (Ni) | 58.0 min | 50.0 min |
| Chromium (Cr) | 20.0-23.0 | 17.0-21.0 |
| Molybdenum (Mo) | 8.0-10.0 | 2.8-3.3 |
| Niobium (Nb) + Tantalum (Ta) | – | 4.75-5.50 |
| Iron (Fe) | 5.0 max | 0.0-21.0 |
| Titanium (Ti) | 0.40 max | 0.65-1.15 |
| Aluminum (Al) | 0.40 max | 0.20-0.80 |
| Cobalt (Co) | 1.0 max | 1.0 max |
| Carbon (C) | 0.10 max | 0.08 max |
| Manganese (Mn) | 0.50 max | 0.35 max |
| Silicon (Si) | 0.50 max | 0.35 max |
| Sulfur (S) | 0.015 max | 0.015 max |
| Phosphorus (P) | 0.015 max | 0.015 max |
Inconel 718 Properties
| Property | Value |
| Density | 8.19 g/cm³ |
| Melting Point | 1260-1340°C (2300-2440°F) |
| Tensile Strength | 1034 MPa (150 ksi) |
| Yield Strength | 724 MPa (105 ksi) |
| Elongation | 12% |
| Modulus of Elasticity | 200 GPa (29.0 x 10^6 psi) |
| Thermal Conductivity | 11.0 W/m·K (at 100°C) |
| Specific Heat Capacity | 447 J/kg·K |
| Coefficient of Thermal Expansion | 13.3 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.22 µΩ·m (at 21°C) |
Inconel 625 Properties
| Property | Value |
| Melting Point | 1290-1350°C (2350-2460°F) |
| Tensile Strength | 827 MPa (120,000 psi) |
| Density | 8.44 g/cm³ |
| Yield Strength (0.2% offset) | 414 MPa (60,000 psi) |
| Elongation | 30% in 2 inches |
| Hardness (HRC) | 20-30 |
| Thermal Conductivity | 11.5 W/m·K (70°F) |
| Coefficient of Thermal Expansion | 13.3 µm/m-°C (20-100°C) |
| Specific Heat Capacity | 442 J/kg·K (20°C) |
| Electrical Resistivity | 1.29 µΩ·m (20°C) |
| Corrosion Resistance | Excellent resistance to corrosion in many environments, including seawater, acids, and oxidizing chemicals. |
Inconel 625 vs Inconel 718: Industrial Applications
Inconel 625 and Inconel 718 are both highly versatile superalloys with unique properties that make them suitable for different applications across various industries.
| Aspect | Inconel 625 | Inconel 718 |
| Chemical Makeup | Primarily nickel and chromium, with additional | Contains nickel, chromium, niobium, and molybdenum, |
| elements like molybdenum and niobium. | among others. | |
| Strength | Offers good strength and toughness, suitable for | Provides superior strength and high-temperature |
| high-temperature applications. | applications, such as aircraft engines. | |
| Corrosion | Excellent corrosion resistance, particularly in | Good corrosion resistance and weldability, making |
| Resistance | acidic environments. | it ideal for harsh environments. |
| Temperature | Can withstand high temperatures, making it | Exhibits excellent resistance to oxidation and |
| Resistance | suitable for heat exchangers and chemical | maintains strength at elevated temperatures. |
| processing equipment. |
Inconel 625 is commonly used in applications that require corrosion resistance, such as chemical processing equipment, marine applications, and aerospace components. Its resistance to sour environments makes it valuable in industries that handle corrosive substances. On the other hand, Inconel 718 has excellent strength and high-temperature resistance, making it ideal for demanding applications such as aircraft engine components, gas turbine components, and high-stress environments in the oil and gas industry. Both alloys have advantages based on their properties, allowing engineers and manufacturers to select the most appropriate material for specific applications.
Conclusion
Choosing between Inconel 625 and Inconel 718 can be difficult, but understanding their properties will make the choice easier. If you need to operate at higher temperatures, choose Inconel 625. For lower temperatures, Inconel 718 is better. Learn about their pros and cons and choose the material that suits your needs.