What Is The Difference Between Inconel 600 And 625 Alloy?

 
Inconel 600 VS 625 Alloy

What is the difference between Inconel 600 and 625 Alloy?

Inconel 625 alloy is not susceptible to chloride stress corrosion cracking and pitting, making it an ideal choice for harsh marine environment applications. Inconel 625 alloy's oxidation resistance exceeds that of Inconel 600 alloy because of its higher chromium and molybdenum content, which allows it to perform well even in extreme temperatures.

What is Inconel 600 used for?

Inconel 600 alloy is used in the electronics field to make parts such as cathode ray tube brackets, thyratron grids, tube supports and springs. The alloy is a standard manufacturing material for nuclear reactors.

inconel-600vsinconel-625

What is the difference between Inconel 625 and INCONEL 725?

INCONEL 625 alloy contains small amounts of cobalt and silver, which are absent in INCONEL 725 alloy. INCONEL 725 alloy has a higher titanium content (1-1.7%, while INCONEL 625 alloy has a maximum of 0.4%), and the rest is made up of iron, while INCONEL 625 alloy has a maximum of 5%.

What are the benefits of Inconel 625?

In addition to high tensile strength, INCONEL 625 also has high creep strength, high rupture strength and excellent weldability. These properties make it suitable for aerospace applications, including duct and exhaust systems, turbine shrouds and seals, and thrust reverser systems.

Equivalent Grades Of Inconel 600 & Inconel 625

 

equivalent-grades-of-inconel-600-and-inconel-625

Equivalent Grades INCONEL 625 INCONEL 600
EN – DIN NiCr 22 Mo 9 Nb NiCr 15 Fe
ASTM – UNS N06625 N06600
W. Nr 2.4856 2.4816
AFNOR NC 22 DNb NC 15 Fe 7 TA

Chemical Composition Of Nickel 600 & 625

 

chemical-composition-of-nickel-600-625

Properties INCONEL 625 INCONEL 600
Sulfur (S) 0 to 0.015 0 to 0.015
Carbon (C) 0 to 0.1 0 to 0.15
Aluminum (Al) 0 to 0.4 -
Manganese (Mn) 0 to 0.5 0 to 1.0
Iron (Fe) 0 to 5.0 6.0 to 10
Molybdenum (Mo) 8.0 to 10 -
Nickel (Ni) 58 to 68.9 72 to 80
Chromium (Cr) 20 to 23 14 to 17
Niobium (Nb) 3.2 to 4.2 -
Cobalt (Co) 0 to 1.0 -
Silicon (Si) 0 to 0.5 0 to 0.5
Titanium (Ti) 0 to 0.4 -
Phosphorus (P) 0 to 0.015 -
Copper (Cu) - 0 to 0.5

Nickel Alloy 600 & 625 Temperature Range

 

nickel-alloy-600--625-temperature-range

Grades Heat Treatment Temperature Range
600 Annealed 1350 °C (2470 °F)
600 Full-Hard 1350 °C (2470 °F)
600 Half-Hard 1350 °C (2470 °F)
600 Hot Worked 1350 °C (2470 °F)
625 Annealed 1290 °C (2350 °F)
625 Solution Treated 1290 °C (2350 °F)

Alloy 600 vs 625 Melting Point

 

 

 

 

 

 
 
 
 
 
 
 
 
 

alloy-600-vs-625-melting-point

Grades Heat Treatment Melting Onset Melting Completion
600 Annealed 1350 °C (2470 °F) 1410 °C (2580 °F)
600 Full-Hard 1350 °C (2470 °F) 1410 °C (2580 °F)
600 Half-Hard 1350 °C (2470 °F) 1410 °C (2580 °F)
600 Hot Worked 1350 °C (2470 °F) 1410 °C (2580 °F)
625 Annealed 1290 °C (2350 °F) 1350 °C (2460 °F)
625 Solution Treated 1290 °C (2350 °F) 1350 °C (2460 °F)

Conclusion

 

Gnee Steel is a supplier of Inconel 600 and 625 Alloy, including tubes, pipes, plates, strips, plates, round bars, flat bars, forged billets, hexagons, wire and extrusions. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Inconel 600 and 625 Alloy tubes, pipes, plates, strips, plates, round bars, flat bars, forged billets, hexagons, wire and extrusions. You are welcome to contact us for a quote at any time at ss@gneesteel.com

Send Inquiry

whatsapp

Phone

E-mail

Inquiry