What Is The Chemical Composition Of 600?

What is the chemical composition of 600?

 

 

Nickel Alloy 600, also sold under the brand name Inconel 600. It is a unique nickel-chromium alloy that is known for its oxidation resistance at higher temperatures. It is highly versatile and can be used in everything from cryogenics to applications that present elevated temperatures up to 2000°F (1093°C). Its high nickel content, a minimum of Ni 72%, combined with its chromium content, provides users of Nickel Alloy 600 a number of benefits including:

Good oxidation resistance at high temperatures
Corrosion resistance to both organic and inorganic compounds
Resistance to chloride-ion stress corrosion cracking
Works well with most alkaline solutions and sulfur compounds
Lower rate of attack from chlorine or hydrogen chloride
Because of its versatility, and because it is the standard engineering material for applications that require resistance to corrosion and heat, a number of different critical industries use Nickel Alloy 600 in their applications. It is a superior choice for:

What is the chemical composition of 600? 600 alloy pipe

Nuclear reactor vessels and heat exchanger tubing
Chemical processing equipment
Heat treat furnace components and fixtures
Gas turbine components including jet engines
Electronic parts
Nickel Alloy 600 and Inconel 600 are readily fabricated (hot or cold) and can be joined using standard welding, brazing, and soldering processes. To be called Nickel Alloy 600 (Inconel 600), an alloy must include the following chemical attributes:

Ni 72%
Cr 14-17%
Fe 6-10%
Mn 1%
Si .5%
Nickel Alloy 600 is available from GNEE group in rod, bar, wire, forging stock, plate, sheet, strip, pipe, and tube. These forms meet or exceed a number of different standards from ASTM, ASME, SAE, AMS, BS, DIN, ISO, QQ, and MIL-DTL.

We stock and sell Nickel Alloy 600 and Inconel 600 in Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon, wire, and extruded section.