What is the chemical composition of 600?
Nickel Alloy 600, also sold under the brand name Inconel 600. It is a unique nickel-chromium alloy that is known for its oxidation resistance at higher temperatures. It is highly versatile and can be used in everything from cryogenics to applications that present elevated temperatures up to 2000°F (1093°C). Its high nickel content, a minimum of Ni 72%, combined with its chromium content, provides users of Nickel Alloy 600 a number of benefits including:
Good oxidation resistance at high temperatures
Corrosion resistance to both organic and inorganic compounds
Resistance to chloride-ion stress corrosion cracking
Works well with most alkaline solutions and sulfur compounds
Lower rate of attack from chlorine or hydrogen chloride
Because of its versatility, and because it is the standard engineering material for applications that require resistance to corrosion and heat, a number of different critical industries use Nickel Alloy 600 in their applications. It is a superior choice for:
Nuclear reactor vessels and heat exchanger tubing
Chemical processing equipment
Heat treat furnace components and fixtures
Gas turbine components including jet engines
Electronic parts
Nickel Alloy 600 and Inconel 600 are readily fabricated (hot or cold) and can be joined using standard welding, brazing, and soldering processes. To be called Nickel Alloy 600 (Inconel 600), an alloy must include the following chemical attributes:


Ni 72%
Cr 14-17%
Fe 6-10%
Mn 1%
Si .5%
Nickel Alloy 600 is available from GNEE group in rod, bar, wire, forging stock, plate, sheet, strip, pipe, and tube. These forms meet or exceed a number of different standards from ASTM, ASME, SAE, AMS, BS, DIN, ISO, QQ, and MIL-DTL.
We stock and sell Nickel Alloy 600 and Inconel 600 in Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon, wire, and extruded section.
Nickel Alloy 600 and Inconel 600 Standards
- Rod, Bar, Wire and Forging Stock
-
-
ASTM B 166/ASME SB 166
ASTM B 564/ASME SB 564
ASME Code Cases 1827 and N-253
SAE/AMS 5665 and 5687
BS 3075NA14 and 3076NA14
DIN 17752, 17753 and 17754
ISO 9723
9724, and 9725
MIL-DTL-23229
QQ-W-390
-
- Plate, Sheet and Strip
-
-
ASTM B 168/ASME SB 168
ASTM B 906/ASME SB 906
ASME Code Cases 1827 and N-253
SAE/AMS 5540
BS 3072NA14 and 3073NA14
DIN 17750
ISO 6208
EN 10095
MIL-DTL-23228
-
- Pipe and Tub
-
-
ASTM B 167/ASME SB 167
ASTM B 163/ASME SB 163
ASTM B 516/ASME SB 516
ASTM B 517/ASME SB 517
ASTM B 751/ASME SB 751
ASTM B 775/ASME SB 775
ASTM B 829/ASME SB 829
ASME Code Cases 1827
N-20, N-253, and N-576
SAE/AMS 5580
DIN 17751
ISO 6207
MIL-DTL-23227
-