What is Monel 400 used for?
Overview
Monel 400 is a nickel-copper alloy that is resistant to high temperature seawater and steam as well as salt and alkaline solutions.
Monel 400 is a nickel-copper alloy that has excellent corrosion resistance in a wide range of media. Monel 400 is characterized by good general corrosion resistance, good weldability, and medium-to-high strength. The alloy has been used in a variety of applications. It has excellent resistance to fast-flowing salt water or seawater. It is particularly resistant when degassed by hydrochloric and hydrofluoric acids. The alloy is slightly magnetic at room temperature. Monel 400 is widely used in the chemical, petroleum, and marine industries.


Characteristics
Corrosion resistance in a wide range of marine and chemical environments. From pure water to non-oxidizing mineral acids, salts, and alkalis.
This alloy is more resistant to nickel under reducing conditions and more resistant than copper under oxidizing conditions, but it does resist reducing media better than oxidizing media.
Good mechanical properties from sub-zero temperatures to temperatures of about 480C.
Good resistance to sulfuric acid and hydrofluoric acid. However, aeration can lead to an accelerated corrosion rate. It can be used to handle hydrochloric acid, but the presence of oxidizing salts greatly accelerates corrosion.
Shows resistance to neutral, alkaline and acidic salts, but poor resistance to oxidizing acidic salts such as ferric chloride.
Excellent resistance to chloride ion stress corrosion cracking.
Applications
Feedwater and steam generator piping.
Brine heaters, seawater scrubbers in tanker inert gas systems.
Sulfuric acid and hydrofluoric acid alkylation units.
Pickling rod heating coils.
Heat exchangers in various industries.
Transfer piping in crude towers in refineries.
Plants for uranium refining and isotope separation in nuclear fuel production.
Pumps and valves for the manufacture of perchloroethylene, chlorinated plastics.
Monoethanolamine (MEA) reboiler tubes.
Cladding of the upper area of crude towers in refineries.
Propeller and pump shafts.