What Is Alloy 2507 Super Duplex Pipe

 

2507 Super Duplex is a high alloy duplex stainless steel with a PRE (pitting resistance equivalent) value of 42.5 minimum. The grade is characterized by very good chloride corrosion resistance, combined with very high mechanical strength. It is particularly suited for use in aggressive environments such as warm chlorinated seawater and acidic chloride-containing media. It is widely used in offshore oil and gas exploration/production and in heat exchangers in petrochemical/chemical processing. The grade is also suitable for hydraulic and instrumentation applications in tropical marine environments.

 

 

Chemical Requirements

Super Duplex 2507 (UNS S32750)
Composition %

C
Carbon

Mn
Manganese

P
Phosphorous

S
Sulfur

Si
Silicon

Ni
Nickel

Cr
Chromium

Mo
Molybdenum

N
Nitrogen

Cu
Copper

0.030 max

1.20 max

0.035 max

0.020 max

0.80 max

6.0–8.0

24.0–26.0

3.0–5.0

0.24–0.32

0.50 max

Dimensional Tolerances

Super Duplex 2507 Stainless Steel

OD

OD Tolerance

Wall Tolerance

≤ .500"

± .005"

± 15%

0.500"–1.500" excl

± .005"

± 10%

Mechanical Properties

Yield Strength:

80 ksi min

Tensile Strength

116 ksi min

Elongation (min 2")

15%

Hardness (Rockwell C Scale)

32 HRC max

 

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia. To learn more about stainless steel products, choose GNEE Steel.