What domestic brand is INCONEL600 equivalent to?
Detailed introduction of Inconel600 high temperature alloy:
Alloy 600 is a nickel-chromium-iron-based solid solution strengthened alloy. It has good high-temperature corrosion resistance and oxidation resistance, excellent hot and cold processing and welding process performance, and has satisfactory thermal strength and high plasticity below 700°C. Alloys can be strengthened by cold working or joined by resistance welding, fusion welding or brazing.
Inconel600 metallographic structure:
When the alloy was treated at 1120°C for 2 hours, there were only TiN nitrides and Cr7C3 carbides. After long-term aging at 870°C and 1500°C, the structure still contained Cr7C3 and TiN, indicating that the alloy's structure was stable.
Inconel600 process performance and requirements:
1. This alloy has good hot working properties, and the heating temperature for steel ingot forging is 1110℃~1140℃.


2. The average grain size of the alloy is closely related to the deformation degree and final forging temperature of the forging.
3. The alloy has good welding properties and can be connected by various methods such as arc welding, argon arc welding, resistance welding and brazing. Large or complex welded structural parts should be annealed at 870°C for 1 hour after welding to eliminate welding. stress.
4. The alloy must be machined after heat treatment. Due to the work hardening of the material, it is advisable to use a lower cutting speed and heavy feed than when processing low-alloy standard austenitic stainless steel, so that it can be machined under the cold work-hardened surface layer. .
Inconel600 main specifications:
Inconel600 seamless pipe, Inconel600 steel plate, Inconel600 round steel, Inconel600 forgings, Inconel600 flange, Inconel600 ring, Inconel600 welded pipe, Inconel600 steel strip, Inconel600 straight bar, Inconel600 wire and supporting welding materials, Inconel600 processed parts.