What Are the Different Types of Inconel?
There are a wide variety of Inconel type alloys (excluding Inconel and Hastelloy). The different types are listed below:
1.Inconel 600
This is the original alloy. It is heat and corrosion resistant and is known for its resistance to high temperature corrosion/oxidation, good hot and cold working properties, good low temperature strength and hot/cold fatigue properties. It has high strength at 650 °C and is suitable for chemical plant components.
2.Inconel 601
The alloy has excellent oxidation resistance and high resistance to carburization at high temperatures. It is beneficial to high temperature organic chemical plants. It resists oxidation in sulfur atmosphere and has good mechanical properties at room and high temperatures. Due to its low carbon content and fine grain structure, it has good resistance to stress corrosion cracking. It has particularly good creep strength at high temperatures (above 500 °C, where other alloys may fail). 601GC is a grain-controlled version of this alloy that offers enhanced properties compared to 601.


3.Inconel 625
This alloy has better corrosion resistance than 600 and 601. It has better performance in maintaining strength and resisting creep from cryogenic temperature to maximum service temperature of 980 °C
4.Inconel 718
This alloy is suitable for precipitation hardening. It has good strength and toughness at temperatures up to 650 °C and good general corrosion/oxidation resistance at all operating temperatures. It is specially formulated for solution treatment or precipitation hardening.
5.Inconel X-750
The alloy has high corrosion and oxidation resistance and good strength below 980 °C. In addition, Inconel X-750 has good low temperature performance and molding properties. Mainly used in aerospace and industrial gas turbine components.
6.Inconel 690
This alloy has greater resistance to chloride corrosion (such as salt water), high temperature/high pressure water stress corrosion, strong oxidizing environment and fluorinated atmosphere corrosion. Mainly used in nitric acid environments, steam generators, and nuclear waste treatment plants.
7.Inconel 792
The alloy's higher aluminum content improves resistance to high-temperature corrosion. It is best suited for use in gas turbine blades and combustor components for chemical rockets.