Apr 02, 2024 Leave a message

Super Duplex Steel S32760 Bright Bar

GNEE Steel is the manufacturer of the wide ranges of the Super Duplex Steel UNS S32760 Stainless Bar. However, we are supplier and exporter of the superior quality of the steel bar to all the global clients. We are providing the best grade bar in various specifications to the clients as per the expectations. National and international quality standards are followed in the manufacturing of the duplex grade bar. Super Duplex Steel UNS S32760 is having various compositions of the alloying elements that provide various properties. Some of the alloying elements which are present in the manufactured stainless steel bar grades are sulfur, molybdenum, phosphorous, manganese, and silicon. However, the grade also requires identical amounts of the carbon and chromium contents to give it corrosion resistance ability. Thus, the grade manufactured bars are interchangeably used in the industrial applications.

ss barss round bar

 

Super Duplex Steel 1.4410 SS Bar is having various characteristics with the presence of the alloying elements. Some of the characteristics features that are there in the manufactured duplex steel bars are corrosion resistance ability, durability, ductility, and many more.


2507 Super Duplex Steel Bars Specification :

Specifications : ASTM A479, ASME SA479
Thickness : 0.5mm to 500mm Diameter
Length : 100 to 6000mm length
Bar Finishing : Bright, Polish & Black
Form : Round Rod, Square Rod, Hex Bar (A/F), Bush Rod, Rectangle Rod, Flat Rod, Wire Mesh
Length : Single Random, Double Random & Cut Length
Rods : 4mm to 350mm dia, wires – 0.5mm to 10mm dia


ASTM A276 Super Duplex Steel S32760 SS Round Bars Equivalent Grades

STANDARD WERKSTOFF NR. UNS
Super Duplex 2507 1.4410 S32760

 

Super Duplex S32760 ASTM A276 Bars Chemical Composition

C Mn Si P S Cr Mo Ni N Fe
0.05 max 1.00 max 1.00 max 0.030 max 0.010 max 24.00 – 26.00 3.00 – 4.00 6.00 – 8.00 0.20 – 0.30 57.61 min

 

Super Duplex WERKSTOFF NR. 1.4410 Stainless Bars Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.8 g/cm3 1350 °C (2460 °F) Psi – 116000 , MPa – 800 Psi – 80000 , MPa – 550 15 %

 

ASTM A276 Super Duplex Steel UNS S32760 Round Bars

ASTM A276 Super Duplex Steel UNS S32760 Round Bars

Super Duplex Steel UNS S32760 Bars

Super Duplex Steel UNS S32760 Bars

Send Inquiry

whatsapp

Phone

E-mail

Inquiry