Research on heat treatment process of high temperature alloys

 

 

Heat treatment process of high temperature alloys refers to a metal heat processing process in which high temperature alloy materials have obtained the expected structure and performance by heating, heat preservation and cooling in the solid state. In recent years, the more in-depth and systematic research on high temperature alloys is solution heat treatment and aging heat treatment. Solution heat treatment refers to the full dissolution temperature of the precipitated phase in the high temperature alloy structure, which is the full dissolution of various unevenly distributed precipitation phases in the alloy into the matrix phase, thereby strengthening the solid solution and improving toughness and corrosion resistance, eliminating residual stress, so as to continue processing and forming, and prepare for the subsequent aging treatment to precipitate uniformly distributed strengthening phases. Aging heat treatment refers to heating and keeping warm for a certain period of time in the temperature range of strengthening phase precipitation, so that the strengthening phase of the high temperature alloy is uniformly precipitated and carbides are evenly distributed, thereby hardening the alloy and improving its strength.

Research on heat treatment process of high temperature alloysResearch on heat treatment process of high temperature alloys

High-temperature alloy GH4145 is a nickel-based age-hardening alloy with [Ni3(Al, Ti, Nb)] as the main strengthening phase, mainly used for 300MW or 600MW steam turbine high and medium pressure inner cylinder flange bolts. After high-temperature operation, this kind of material bolts will undergo microstructure and borrowing configuration changes, precipitation of strengthening phases, etc., resulting in a decrease in the creep and durability of the material. In order to improve its performance, the bolts with a hardness value of 333HBW after operation are subjected to recovery heat treatment. The heat treatment process is solid solution + two aging, and the solid solution process is 1130℃×1h oil cooling; the first aging is 845℃×24h, and the second aging is 707℃×20h air cooling. After the recovery heat treatment of the bolts with excessive hardness values ​​using this process, the hardness value is reduced to the standard requirement range. Although the strength value has a certain degree of decrease, the plasticity and toughness are significantly improved, proving that the recovery heat treatment process is very effective.

GH4169 alloy is a high-strength nickel-chromium-iron-based high-temperature alloy containing Nb, which is mainly used to manufacture high-temperature components of aircraft engines. The effect of heat treatment system on the microstructure and properties of GH4169 cold-rolled blades. The 970-995℃ softening treatment system is adopted, and the intermediate treatment and solution aging treatment are carried out after the softening treatment. The intermediate treatment system is 900℃ air cooling, and the solution aging treatment system is 1010℃ air cooling + 720℃×8h furnace cooling to 620℃×8h air cooling. Softening treatment can significantly reduce the hardness, which is conducive to the second cold rolling; using 995℃ for softening treatment can obtain a better softening effect and has no effect on the alloy microstructure and properties; after the GH4169 alloy is cold-rolled and deformed, the softening treatment has little effect on the mechanical properties, while the intermediate treatment and the final solution aging heat treatment are important processes that determine the mechanical properties.

High-temperature alloys are heat treated under strictly controlled heating and cooling conditions to achieve the required performance or service life by changing the internal microstructure of the material. With the application of new high-temperature alloy materials and the high requirements for alloy performance during use, heat treatment technology is an indispensable process. In recent years, the heat treatment technology of high-temperature alloys has been continuously developing, and its development trends are as follows:

(1) The heat treatment system, together with the alloy composition design and other processes, enables the high-temperature alloy to achieve the best performance state in order to achieve the best performance match.

(2) Computer simulation is combined with heat treatment technology to conduct in-depth research on the deformation and heat treatment of the alloy. Study the heat treatment process control system, realize process innovation while paying attention to equipment renewal, and develop equipment and technology in parallel.

(3) The mutual transformation relationship and phase transformation mechanism between the various precipitated phases of the alloy during service and heat treatment are not very clear, and in-depth research is needed.

(4) In-depth research on the appropriate quenching medium for high-temperature alloys and improving the quenching process will be the focus of future heat treatment technology research.

(5) Vacuum heat treatment technology has the advantages of no oxidation, no decarburization and small distortion, and its application in industries such as aerospace will become more and more extensive.

(6) Plasma surface treatment has the characteristics of wear resistance, small distortion, good appearance and no blind area, and will be widely used in high-temperature alloys, including ion nitriding, ion nitrocarburizing, ion carburizing and other technologies.