Feb 19, 2024 Leave a message

Is Nickel Alloy The Same As Hastelloy?

Is nickel alloy the same as hastelloy?

 

Hastelloy C-276, also sold as Nickel Alloy C-276, is a nickel-molybdenum-chromium deformed alloy. Hastelloy C-276 is ideally suited where protection from severe and localized corrosion is required. Other important properties of the alloy Nickel Alloy C-276 and Hastelloy C-276 include its resistance to oxidizing agents such as:

Ferric chloride and copper chloride
Organic and inorganic thermal contamination media
Chlorine (wet chlorine)
seawater
acid
hypochlorite
carbon dioxide

Is nickel alloy the same as hastelloy?

Is nickel alloy the same as hastelloy?

Hastelloy C-276 and Nickel Alloy C-276 Applications
Additionally, Nickel Alloy C-276 and Hastelloy C-276 can be welded using all common welding methods (oxyacetylene is not recommended). Because of Hastelloy C-276's excellent corrosion resistance, it is used in a wide range of critical applications across a variety of industries, including:

Almost everything related to sulfuric acid (heat exchangers, evaporators, filters and mixers)
Bleaching units and digesters for paper and pulp manufacturing
Components used around sour gases
Marine Engineering
waste disposal
pollution control
Chemical composition of Hastelloy C-276 and Nickel Alloy C-276
Its chemical composition makes it unique and includes:

Nickel 57%
Molybdenum 15-17%
Chromium 14.5-16.5%
Iron 4-7%
Water 3-4.5%
Manganese 1% or less
Cobalt content up to 2.5%
Vmax .35%
Max Silicon .08
At Continental Steel, we distribute Nickel Alloy C-276 and Hastelloy C-276 including fittings, plates, tubes, rounds, strips, plates and tubes. All of the plants we work with offer Nickel Alloy C-276 and Hastelloy C-276 that meet or exceed industry standards, including the ASME Boiler and Pressure Vessel Code.

 

 

 

 