Is Inconel X750 magnetic?
Alloy X750
Industry Name Alloy X-750X750Inconel Alloy X-750
Material Special Specialty Steel
Specification AMS 5542 AMS 5598 AMS 5667 AMS 5670 UNS N07750
Applications Aerospace Components Machined Components Industrial
Features Excellent Corrosion Resistance High Strength at Elevated Temperatures Limited Weldability


Alloy X750 is a precipitation hardened austenitic nickel-chromium alloy. It is similar to Inconel 600, but is classified as PH and has additions of aluminum and titanium. It has good general corrosion and oxidation resistance. Alloy X-750 is non-magnetic and resists a wide range of industrial corrosives in both reducing and oxidizing conditions. In addition, Alloy X750 has excellent resistance to chloride stress corrosion cracking in the fully age-hardened condition. For more information on Alloy X750, check out our video transcript on the subject! Watch below.
| Property | Value |
|---|---|
| .2% Yield Strength | 141 ksi |
| Elongation | 23.6 % |
| Ultimate Tensile Strength | 192 ksi |
| Element | Min | Max |
|---|---|---|
| Al | .8 | |
| C | - | .08 |
| Cb | 1.0 | |
| Cr | - | 16.0 |
| Fe | 8 | |
| Mn | - | .35 |
| Ni | 70.0 | Bal |
| Si | - | .35 |
| Ti | 2.5 |