Jan 08, 2024 Leave a message

Introduction To The Characteristics Of Incoloy 800 Alloy

Introduction to the characteristics of Incoloy 800 alloy

 

Incoloy800 Overview and Application

Incoloy800 high temperature alloy is a Ni-Fe-Cr series iron-nickel-based corrosion-resistant alloy with Ni and Cr as the main components. Incoloy800 is in the austenite single zone after rapid cooling from high temperature. Therefore, the use state is a single austenite structure. This alloy has a high chromium content and sufficient nickel content, so it has high high temperature corrosion resistance, excellent stress corrosion resistance and oxidation resistance. It is often used in nuclear power evaporation heat transfer tubes and ultrasonic evaporation heat transfer tubes with temperatures above 700°C. Supercritical generator sets, high-temperature equipment in the petrochemical industry (such as catalytic tubes, convection tubes, cracking tubes, reformers and pigtail tubes) have excellent stress resistance in chloride, low-concentration NaOH aqueous solutions and high-temperature and high-pressure water. Corrosion cracking performance, so it is used to manufacture equipment resistant to stress corrosion cracking. Incoloy800 can be used in chemical industry nuclear generator nitric acid coolers, acetic anhydride cracking tube heat exchange equipment and heat exchange tubes under softening annealing conditions up to 600°C.

Introduction to the characteristics of Incoloy 800 alloy

Introduction to the characteristics of Incoloy 800 alloy

Features of Incoloy800

Good corrosion resistance and heat resistance, corrosion resistance is better than general austenitic stainless steel, and better than Incolo 600 alloy; in manufacturing corrosion-resistant stress cracking equipment, it is better than Incolo 600 and Monel 400 alloy. It has good mechanical properties at low and high temperatures up to 800°C, good resistance to oxidation, reduction and nitriding, good processability, and can also be used in environments that require resistance to moisture corrosion. However, for application temperatures above 600°C, it is recommended to use solution annealed Incoloy800H. Incoloy800 is resistant to a variety of corrosive media. For wet corrosive environments, the alloy's higher nickel content gives it good resistance to stress cracking corrosion. The increased chromium content enhances resistance to pitting and crevice corrosion. The alloy shows good resistance to nitric and organic acids, but has limited resistance to sulfuric and hydrochloric acids, and pitting corrosion may occur in halogen acids. This material has good corrosion resistance. It is also resistant to fresh water and steam as well as mixtures of steam, air and water and has excellent resistance to oxidation and carburization. Resistant to hydrogen, nitrogen and corrosion.

Incoloy800 is an alloy that usually contains 15-25% Cr, 30-45% nickel, and small amounts of aluminum and titanium. Incoloy800/alloy800 has good resistance to stress corrosion cracking in water chloride, corrosion resistance to steam, air and carbon dioxide mixtures, and good corrosion resistance to organic acids such as HNO3, HCOOH, CH3COOH, CH3CH2COOH. . It is often used to make various pipes, heat exchangers, liquid distillers, etc. in the petrochemical industry and various heat treatment furnaces.
​