INCONEL 600 fasteners are a nickel-chromium alloy designed for extreme temperature applications, from cryogenics to 1100°C (2000°F). The alloy's nominal composition is 72% nickel, 14-17% chromium, 5-9% iron, and trace amounts of other elements such as manganese, silicon, and titanium.
What is Inconel 600 made of?
Inconel 600 is a nickel-chromium alloy that offers good oxidation resistance at high temperatures and good resistance to carburizing and chloride-containing environments. Inconel 600 is a nickel-chromium alloy designed for use in temperatures ranging from cryogenic to 2000°F (1093°C).

Inconel 600 Fasteners Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
Inconel 600 Fasteners Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
Applications of Inconel 600 Fasteners
Inconel 600 fasteners are widely used in numerous applications due to their excellent corrosion resistance and high-temperature performance. Inconel 600 pins are most commonly used in oil and gas production plants, petrochemical processing plants, chemical processing equipment, aerospace components, offshore engineering, and heat exchangers.
In addition to being extremely resistant to corrosion from acidic media such as sulfurous acid and hydrochloric acid, 600 fasteners also exhibit excellent oxidation resistance at temperatures up to 1500°F (815°C). Furthermore, Inconel 600 has good processing characteristics, making it ideal for welding or forming into custom shapes.
Inconel 600 Fastener Characteristics
600 fasteners' reliable performance even in extreme temperatures and harsh environments makes them a preferred choice across many industries. Inconel 600 pins are widely used in a variety of projects, from heat exchangers and piping to turbines, valves, pumps, and pressure vessels.
600 fasteners offer a combination of strength and corrosion resistance, making them ideal for a wide range of applications requiring reliable performance in extreme temperatures.
Overall, their superior corrosion resistance and high-temperature performance make 600 fasteners one of the most trusted materials available today. They are used in a wide range of industries, including oil and gas production plants, petrochemical processing plants, chemical processing equipment, aerospace components, offshore engineering, and heat exchangers.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications, and we can provide customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.