Inconel 600 Mechanical Properties And Implementation Standards in Various Countries

Inconel 600 mechanical properties and implementation standards in various countries

 

 

Overview of Inconel 600 characteristics and application areas:

This alloy is a nickel-chromium-iron based solid solution strengthened alloy with good high temperature corrosion resistance and oxidation resistance, excellent hot and cold processing and welding performance, and satisfactory thermal strength and high plasticity below 700℃. The alloy can be strengthened by cold working, and can also be connected by resistance welding, fusion welding or brazing. It is suitable for making anti-oxidation parts that bear low loads below 1100℃

 

Similar grades of Inconel 600:

Japan: NCF600 NCF600TP NCF600TB

USA: Inconel600 UNS6600 NO6600

China: GH600

France: NC15F

Germany: 2.4816 NiCr15Fe

UK: NA14

 

Chemical composition of Inconel 600:

Nickel Ni: ≥72.00
Chromium Cr: 14.0~17.0
Iron Fe: 6.0~10.0
Carbon C: ≤0.15
Manganese Mn: ≤1.00
Silicon Si: ≤0.50
Sulfur S: ≤0.015
Phosphorus P: ≤0.030
Copper Cu: ≤0.50

Inconel 600 mechanical properties and implementation standards in various countriesInconel 600 mechanical properties and implementation standards in various countries

Inconel600 Mechanical properties:

German mechanical properties:

Solid solution state:
Tensile strength Rm/MPa: 500
Yield strength Re1 or Rp0.2/MPa: 200
Elongation A/%: 35
Brinell hardness HBS: ≥185

Soft state:
Tensile strength Rm/MPa: 550
Yield strength Re1 or Rp0.2/MPa: 180
Elongation A/%: 30
Brinell hardness HBS: ≥195

 

Inconel600 metallographic structure:

The alloy is treated at 1120℃ for 2h, and only TiN nitride and Cr7C3 type carbide are present. After long-term aging at 870℃ and 1500℃, the organization is still Cr7C3 and TiN, indicating that the organization of the alloy is stable.

 

Inconel600 process performance and requirements:

1. The alloy has good hot working performance, and the ingot forging heating temperature is 1110℃~1140℃.
2. The average grain size of the alloy is closely related to the degree of deformation and final forging temperature of the forging.
3. The alloy has good welding performance and can be connected by various methods such as arc welding, argon arc welding, resistance welding and brazing. Large or complex welded structures should be annealed at 870℃ for 1h after fusion welding to eliminate welding stress.
4. The alloy must be machined after heat treatment. Due to the work hardening of the material, it is advisable to use a lower cutting speed and heavy feed than the standard austenitic stainless steel to machine into the cold-hardened surface layer.

 

Japanese standards:

Seamless pipe: JIS G4903-1991 JIS G4904-1991
Plate: JIS G4902-1991
Bar: JIS G4901-1999

German standards:

DIN 17742-2002
Plate: DIN 17750-2002
Pipe: DIN 17751-2002
Bar: DIN 17752-2002

Japanese mechanical properties:

Tensile strength Rm/MPa: 550
Yield strength Re1 or Rp0.2/MPa: 205
Elongation A /%: 30
Brinell hardness HBS: ≥179

American implementation standard:

Seamless pipe: ASTM B167-05a ASTM B163-04
Welded pipe: ASTM B516-03 ASTM B517-05
Plate: ASTM B168-01 (2005)
Bar: ASTM B166-04

Inconel 600 mechanical properties and implementation standards in various countriesInconel 600 mechanical properties and implementation standards in various countries

Inconel600 physical properties:

Density g/cm3: 8.43
Melting point ℃: 1370-1430
Thermal conductivity λ/(W/m•℃): 12.85(100℃)
Specific heat capacity J/kg•℃: 435
Elastic modulus GPa: 205
Shear modulus GPa: 76
Resistivity μΩ•m: 1.05
Poisson's ratio: 0.34
Linear expansion coefficient a/10-6℃-1 :12.35(20~100℃)

 

US Mechanical Properties:

Seamless pipe hot working annealing ≤Φ127:
Tensile strength Rm/MPa: ≥550
Yield strength Rel or Rp0.2/MPa: ≥205
Flexural strength A/%: ≥35
Seamless pipe hot working annealing>Φ127:
Tensile strength Rm/MPa: ≥515
Yield strength Rel or Rp0.2/MPa: ≥17 0
Flexural strength A/%: ≥35
Seamless pipe cold working annealing ≤Φ127:
Tensile strength Rm/MPa: ≥550
Yield strength Rel or Rp0.2/MPa: ≥240
Flexural strength A/%: ≥30
Seamless pipe cold working annealing>Φ127:
Tensile strength Rm/MPa: ≥550
Yield strength Rel or Rp0.2/MPa: ≥205
Flexural strength A/%: ≥35