Feb 20, 2025 Leave a message

Incoloy Alloy 800 Vs 800H

Incoloy Alloy 800 vs 800H

 

Incoloy Alloy 800 is an alloy containing a small amount of aluminum and titanium and a high content of chromium and nickel. Its Cr content is 15-25% and Ni content is 30-45%. Incoloy 800H is an iron nickel base alloy with a chromium content of 12%.

The different carbon content of Incoloy800 and Incoloy800H makes them very different. The carbon content of INCOLOY ALLOY 800 is below 0.1, and the carbon content of Incoloy 800H is 0.05-0.1.

incoloy alloy round tubeincoloy pipe

Chemical composition:

Alloy

Chemical

element

Cr

Ni

C

Mn

Cu

Fe

Si

S

AI

Ti

800

min

15

30

-

-

-

margin

-

-

0.15

0.15

max

25

35

0.10

1.5

0.75

margin

1

0.015

0.60

0.60

800H

min

19

30

0.05

-

-

margin

-

-

0.15

0.15

max

23

35

0.10

1.5

0.75

margin

1

0.015

0.60

0.60

 

Physical properties:

Alloy

density

melting point

tensile strength

yield strength

Elongation

800

8.0 g/cm3

1350~1400℃

500Rm N/mm2

210RP0.2N/mm2

35%

800H

8.0 g/cm3

1350~1400℃

450Rm N/mm2

180RP0.2N/mm2

35%

 

Same characteristics:
1. Both have good corrosion resistance
2. Good processability
3. Excellent stress corrosion resistance


Applications:

Nitric acid condensers.

Steam heating tubes.

​Heating element tubes.

Send Inquiry