High Temperature Strength Of Inconel Alloys

High Temperature Strength of Inconel Alloys

 

The strength of superalloys is improved by solid solution strengthening and precipitation strengthening or age hardening. The heat treatment used depends on the specific high temperature alloy.

These techniques combine nickel with varying amounts of niobium to form gamma bis (gamma). This intermetallic compound produces tiny cubic crystals that prevent creep deformation and slip at high temperatures.

The formation of these crystals increases over time, especially after exposing the alloy to temperatures of 1,560°F (850°C) and above for 3-72 hours. This thick passivating oxide layer allows the metal to remain exceptionally strong over a wide range of temperatures.

High Temperature Strength of Inconel Alloys

High Temperature Strength of Inconel Alloys

The following is an overview of the mechanical properties of Inconel 718 sheet after precipitation heat treatment.

Yield Strength in Annealed Condition (Minimum Offset 0.2%): 80,000 psi (550 MPa)
Ultimate tensile strength (minimum): 140,000 psi (965 MPa)
Elongation (minimum): 30 (% of 2 inches)
Coefficient of thermal expansion from 77°F to 1400°F: 8.9
Given the high strength of superalloys, there are some key machine considerations that must be taken into account when cutting them. Their high temperature resistance often adds extra heat to cutting tools, reducing their performance. Adding special heat-resistant blades or coatings to the machining process helps the machine hold up better during the cutting process.

 