Incoloy 800H pipe is a high temperature nickel-iron-chromium alloy known for its excellent creep and rupture strength for demanding applications. It is essentially an enhanced version of Incoloy 800, with excellent performance at high temperatures due to controlled carbon content and high temperature annealing. This makes it a top choice for heat exchangers, furnace components and other equipment exposed to high temperatures and corrosive environments.

Incoloy 800H Pipe

What is INCOLOY 800 Pipe?

 

INCOLOY 800 Pipe

Incoloy 800 Pipe is a nickel-iron-chromium alloy pipe that has good strength and excellent resistance to oxidation and carburization in high temperature environments. It has excellent corrosion and heat resistance, making it an ideal choice for applications such as petroleum refining, chemical processing, and power generation.

Alloy 800h tube chemical composition

Grade Nickel Carbon Manganese Silicon Iron Sulfur Chromium
Incoloy 800H 30.0-35.0 0.05-1.00 1.5 1.0 39.5 0.015 23.0

Mechanical properties of Incoloy 800H seamless tube

Grade Tensile Strength Yield Strength (0.2%Offset) Elongation
(per square inch) (megapascal) (per square inch) (megapascal) %
Incoloy 800H 75000 520 30000 205 30

Pressure rating of nickel alloy 800h pipe

Outside Diameter of the Pipe(inches) Pipewall Thickness (inches)
.028 .035 .049 .065 .083 .095 .109 .120
Working Pressure (pounds per square inch gauge)
1/8 7900 10100 – – – – – –
1/4 3700 4800 7000 9500 – – – –
5/16 – 3700 5400 7300 – – – –
3/8 – 3100 4400 6100 – – – –
1/2 – 2300 3200 4400 – – – –
3/4 – – 2200 3000 4000 4600 – –
1 – – – 2200 2900 3400 3900 4300
Gnee Steel

 

About Gnee Steel

Gnee Steel is a company specializing in the production of various nickel-based alloys, nickel 201, nickel202, hastelloy c-276, hastelloy c-22, hastelloy b, hastelloy c-4, Inconel alloy 600, Inconel 625, Inconel 718, Inconel x-750, incoloy alloy 800, incoloy 800H/HT, incoloy 825, monel alloy 400, monel k500 and high temperature alloy materials. It specializes in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, electric power, automobile, nuclear energy and other fields, and can provide customized alloy material solutions according to customer needs. If you need to know the alloy material price consultation or provide customized alloy material solutions, you are welcome to contact us at any time to get a quote at ss@gneesteel.com