ASTM B444 GR.2 Gr.1 INCONEL 625 Heat Exchanger/Boiler Tubes

 
ASTM B444 GR.2 Gr.1 INCONEL 625 Heat Exchanger/Boiler Tubes
ASTM B444 GR2 Gr1 INCONEL 625 Heat ExchangerBoiler Tubes
01

ASTM B444 GR.2 Gr.1 INCONEL 625 Heat Exchanger/Boiler Tubes

ASTM B444 Gr.1/Gr.2 Inconel 625 heat exchanger and boiler tubes are high-strength, nickel-based, seamless superalloy tubes designed for extreme, corrosive, and high-temperature environments. Designated UNS N06625, this alloy is stabilized with niobium for enhanced resistance to intergranular corrosion. It also offers excellent mechanical strength, creep resistance, and toughness over a wide temperature range. Grade 1 is annealed, while Grade 2 is solution annealed. These tubes are suitable for critical applications in industries such as chemical processing, oil and gas, offshore, and nuclear power.

02

What is the difference between Inconel 625 Grade 1 and Grade 2?

Grade 1 is typically annealed at around 1600°F to 1800°F (approximately 871°C to 982°C) to provide good ductility and corrosion resistance while maintaining higher strength than Grade 2. Grade 2 is heat treated above 2000°F (approximately 1093°C) to enhance creep and stress-rupture resistance while maintaining corrosion resistance.

Inconel 625 Grade 1 And Grade 2
 

ASTM B444 GR.2 / GR.1 Inconel 625 seamless pipe is a high-strength nickel-based high-temperature alloy designed for extreme environments where resistance to heat, corrosion, and mechanical stress is critical. It offers high strength, excellent mechanical strength, and toughness even at elevated temperatures. It also exhibits outstanding resistance to oxidation and scaling at elevated temperatures. Its seamless construction ensures uniform strength and structural integrity, with no welds, thus reducing potential weak points.

 

ASTM B444 Grade 1 and Grade 2

ASTM B444 has two grades, each with different heat treatment conditions. ASTM B444 Grade 1 pipe is annealed and can typically be used at temperatures up to 593°C.

Grade 2 pipe is solution annealed and can be used at temperatures above 593°C. ASTM B444 Grade 2 pipe is suitable for applications where creep and rupture resistance are primary requirements. Unless otherwise specified, manufacturers typically provide Grade 1 pipe.

 

Chemical Composition of ASTM B444 UNS N06625 Nickel Alloy Tubes (Weight %)

Element Content (Min - Max)
Nickel (Ni) ≥ 58.00
Manganese (Mn) ≤ 0.50
Phosphorus (P) ≤ 0.015
Sulfur (S) ≤ 0.015*
Silicon (Si) ≤ 0.50
Chromium (Cr) 20.00 - 23.00
Molybdenum (Mo) 8.00 - 10.00
Carbon (C) ≤ 0.10
Cobalt (Co) ≤ 1.00
Iron (Fe) ≤ 5.00
Aluminum (Al) ≤ 0.40
Titanium (Ti) ≤ 0.40
Niobium + Tantalum (Nb+Ta) 3.15 - 4.15

 

Mechanical Properties of ASTM B444 UNS N06625 Nickel Alloy Tubes

Grade Tensile Strength (MPa, min) Yield Strength (MPa, min) Elongation (%, min)
Grade 1 827 414 30
Grade 2 690 276 30

 

Material Properties and Composition
Alloy Type: Nickel-chromium-molybdenum-niobium (niobium) alloy, also known as Alloy 625 or Inconel 625.
Stability: The addition of niobium prevents sensitization and helps protect against intergranular corrosion.
Strength: High tensile and yield strength, as well as excellent mechanical strength and toughness, even at elevated temperatures.
Corrosion Resistance: Excellent resistance to a wide range of corrosive conditions, including pitting, crevice corrosion, stress corrosion, and general corrosion, in both marine and non-marine environments.
Temperature Performance: Excellent resistance to oxidation and scaling at elevated temperatures, with excellent performance even at very low temperatures.

 

Grades and Heat Treatment
ASTM B444: Specifies the standard for cold-worked seamless tubing of these nickel alloys.
Grade 1: Tubes are supplied in the annealed condition for service temperatures up to 1100°F (593°C).
Grade 2: Tubes are supplied in the solution annealed condition, offering enhanced properties for more demanding applications.

 

Heat Exchanger and Boiler Applications
Corrosive Media: Used in harsh or highly acidic environments where other materials may fail.
High-Temperature: Suitable for high-temperature processes, ideal for boiler and superheater tubing.
High-Pressure: Its seamless construction and high strength make it well-suited for high-pressure applications.

 

Industries and Applications
Chemical Processing: Used in the chemical processing industry due to its acid resistance.
Oil and Gas: Suitable for offshore oil and gas applications due to its toughness in high-stress and corrosive marine environments.
Aerospace: Its ability to withstand high and low temperatures and stresses makes it a top choice for aerospace applications.
Nuclear: Its high strength and weldability make it suitable for critical uses in the nuclear industry.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry