ASTM B443 UNS N06625 Annealed Alloy Plate

What is ASTM B443?

ASTM B443 is a standard specification for nickel-chromium-molybdenum-niobium and nickel-chromium-molybdenum-silicon alloy plates, sheets, and strips. It specifies their chemical composition, mechanical properties, and permissible tolerances, and is used in the manufacture of high-performance metal products for use in harsh environments, such as Inconel 625 alloy..

 

What is ASTM B443 UNS N06625 Annealed Alloy Plate?

ASTM B443 UNS N06625 annealed alloy plate refers to a UNS N06625 nickel-based alloy plate (Grade 1) manufactured to ASTM B443 standards, which has undergone annealing at a minimum of 871°C (1600°F) followed by rapid cooling.
GNEE supplies ASTM B443 UNS N06625 annealed plates with a minimum tensile strength of 827 MPa and a minimum 0.2% yield strength of 414 MPa for cold-rolled sheets and strips, while hot-rolled plates (up to 70 mm thick) have a minimum tensile strength of 758 MPa and a minimum yield strength of 379 MPa. All specifications have a minimum elongation of 30%. Suitable for use in environments up to 593°C (1100°F), it exhibits excellent resistance to chloride corrosion and strong corrosive chemicals, and possesses good ductility and formability. Therefore, it is widely used in marine engineering, chemical industry, and other fields requiring reliable corrosion resistance and ease of processing.

 

ASTM B443 UNS N06625 Annealed Alloy Plate

 

Inconel 625 Material Specification: ASTM B443/ ASME SB443 625 Plate Stock Available

Inconel Grade: Inconel 625 (UNS N06625, Alloy 625, 2.4856)

Inconel 625 Plate Thickness: 7 gauge to 28 gauge or 3.664mm to .321mm

Inconel 625 Plate Width Range: 30" to 240"

Inconel 625 Plate Length Range: Up to144" Non-Standard or Longer Lengths Available Upon Request

Inconel 625 Plate Finishes: 2D, 2B, 4Pol, BA, X10, XL, Buff, XL Blend S, SATIN (Met with Plastic Coated), NO (8), Hairline, NO.1, NO.4, Mirror Finish

Inconel 625 Plate Processing: Shearing to Custom Sizes

Inconel 625 Plate Form: Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange)

 

ASTM B443 UNS N06625  Chemical Requirements

Element Min % Max %
Carbon – 0.10%
Manganese – 0.50%
Silicon – 0.50%
Phosphorus – 0.015%
Sulfur – 0.015%
Chromium 20.00% 23.00%
Molybdenum 8.00% 10.00%
Columbium (Niobium) 3.15% 4.15%
Cobalt – 1.00%
Titanium – 0.40%
Aluminum – 0.40%
Iron – 5.00%
Nickel remainder –

 

ASTM B443 Inconel 625 Mechanical Properties

Property Metric Imperial
Hardness, Rockwell B (typical annealed) 95 95
Tensile strength (for flat products <4″ thickness) ≥ 827 MPa ≥ 120,000 psi
Yield strength (for flat products <4″ thickness) ≥ 414 MPa ≥ 60,000 psi
Elongation at break (typical annealed) 45% 45%

 

ASTM B443 Inconel 625 Physical properties

Property Inconel 625 Inconel 600
Tensile Strength Psi – 135,000 , MPa – 930 Psi – 95,000 , MPa – 655
Yield Strength (0.2% Offset) Psi – 75,000 , MPa – 517 Psi – 45,000 , MPa – 310
Elongation 42.5 % 40 %

 

Nickel Alloy 625 Sheet price List

Price of Inconel 625 UNS N06625 Flat Plate Alloy 625 Sheet Price in USD
Inconel Alloy 625 Lcf,vm-esr,type0,cr Sheet In Coil,cr,ann,0.0098,22.2441 Sixe: 25mm 565mm Coil USD 40.57
Ams 5879 Uns No6626 Inconel Alloy 625 Lcf Cr Sheet Anneal 0.250mm Thk Size: 565 Mm Width Coil USD 10362.78
Inconel 625 Sheet Sq Metre (16 Sheets) (Mat-002a) 32 Pcs USD 8681.37
Sheet Of 0.25mm Thick Alloy 625 (Inconel) Astm B 443(Nickelalloy Sheet) USD 44.48

 

UNS N06625 nickel-based alloy plates are manufactured in strict accordance with international and national standards such as ASTM, ASME, JIS, DIN, ASTM B443, and ASME SB 443. The products are available in various sizes with widths ranging from 1000 mm to 3500 mm, thicknesses from 4 mm to 100 mm, and lengths from 2000 mm to 6000 mm. Customized orders are also accepted to meet individual customer needs.

 Inconel 625 UNS N06625 Flat Plate in stock

625 Inconel Plates UNS N06625 Inconel 625 Rolling Plates
ASTM B443 Alloy 625 Chequered Plates Alloy Inconel 625 Quarto Plates
UNS N06625 Inconel 625 Cold Rolled Plates Alloy Inconel 625 Bbq Plates
Alloy Inconel 625 Hot Rolled Plates ASTM B443 Alloy 625 Perforated Plates
Alloy Inconel 625 Plate Mill Finish Inconel 625 Din 2.4856 Thin Plate
ASTM B443 Alloy 625 Plate 2b Finish Alloy 625 Nickel Diamond Plates

The products are carefully packaged in wooden crates and boxes to ensure safe transportation. All UNS N06625 sheets undergo rigorous testing and quality inspection and are supplied with test certificates to guarantee quality.

UNS N06625 Inconel 625 Cold Rolled Plates